Literature DB >> 22778494

Overview: Damage resistance of graded ceramic restorative materials.

Yu Zhang1.   

Abstract

Improving mechanical response of materials is of great interest in a wide range of disciplines, including biomechanics, tribology, geology, optoelectronics, and nanotechnology. It has been long recognized that spatial gradients in surface composition and structure can improve the mechanical integrity of a material. This review surveys recent results of sliding-contact, flexural, and fatigue tests on graded ceramic materials from our laboratories and elsewhere. Although our findings are examined in the context of possible applications for next-generation, graded all-ceramic dental restorations, implications of our studies have broad impact on biomedical, civil, structural, and an array of other engineering applications.

Entities:  

Year:  2012        PMID: 22778494      PMCID: PMC3390941          DOI: 10.1016/j.jeurceramsoc.2012.02.020

Source DB:  PubMed          Journal:  J Eur Ceram Soc        ISSN: 0955-2219            Impact factor:   5.302


  36 in total

Review 1.  Clinically relevant approach to failure testing of all-ceramic restorations.

Authors:  J R Kelly
Journal:  J Prosthet Dent       Date:  1999-06       Impact factor: 3.426

2.  All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2-year clinical study.

Authors:  P Vult von Steyern; P Carlson; K Nilner
Journal:  J Oral Rehabil       Date:  2005-03       Impact factor: 3.837

3.  Failure analysis of ceramic clinical cases using qualitative fractography.

Authors:  Susanne S Scherrer; Janet B Quinn; George D Quinn; J Robert Kelly
Journal:  Int J Prosthodont       Date:  2006 Mar-Apr       Impact factor: 1.681

4.  All-ceramic two- to five-unit implant-supported reconstructions. A randomized, prospective clinical trial.

Authors:  Christel Larsson; Per Vult von Steyern; Bo Sunzel; Krister Nilner
Journal:  Swed Dent J       Date:  2006

5.  Clinical behavior of zirconia-based fixed partial dentures made of DC-Zirkon: 3-year results.

Authors:  Joachim Tinschert; Karen A Schulze; Gerd Natt; Peter Latzke; Nicole Heussen; Hubertus Spiekermann
Journal:  Int J Prosthodont       Date:  2008 May-Jun       Impact factor: 1.681

6.  Improving fatigue damage resistance of alumina through surface grading.

Authors:  L Ren; L Liu; S Bhowmick; Y B Gerbig; M N Janal; V P Thompson; Y Zhang
Journal:  J Dent Res       Date:  2011-05-09       Impact factor: 6.116

7.  A prospective study of implant-supported full-arch yttria-stabilized tetragonal zirconia polycrystal mandibular fixed dental prostheses: three-year results.

Authors:  Christel Larsson; Per Vult von Steyern; Krister Nilner
Journal:  Int J Prosthodont       Date:  2010 Jul-Aug       Impact factor: 1.681

8.  Graded zirconia glass for resistance to veneer fracture.

Authors:  Y Zhang; J W Kim
Journal:  J Dent Res       Date:  2010-07-22       Impact factor: 6.116

9.  HIP zirconia fixed partial dentures--clinical results after 3 years of clinical service.

Authors:  Daniel Edelhoff; Beuer Florian; Weber Florian; Christine Johnen
Journal:  Quintessence Int       Date:  2008-06       Impact factor: 1.677

10.  Clinical performance of extended zirconia frameworks for fixed dental prostheses: two-year results.

Authors:  M Schmitter; K Mussotter; P Rammelsberg; T Stober; B Ohlmann; O Gabbert
Journal:  J Oral Rehabil       Date:  2009-06-02       Impact factor: 3.837

View more
  18 in total

1.  On the interfacial fracture of porcelain/zirconia and graded zirconia dental structures.

Authors:  Herzl Chai; James J-W Lee; Adam J Mieleszko; Stephen J Chu; Yu Zhang
Journal:  Acta Biomater       Date:  2014-04-24       Impact factor: 8.947

Review 2.  Zirconia surface modifications for implant dentistry.

Authors:  Fernanda H Schünemann; María E Galárraga-Vinueza; Ricardo Magini; Márcio Fredel; Filipe Silva; Júlio C M Souza; Yu Zhang; Bruno Henriques
Journal:  Mater Sci Eng C Mater Biol Appl       Date:  2019-01-16       Impact factor: 7.328

3.  Wear Behavior of Graded Glass/Zirconia Crowns and Their Antagonists.

Authors:  M R Kaizer; S Bano; M Borba; V Garg; M B F Dos Santos; Y Zhang
Journal:  J Dent Res       Date:  2019-02-11       Impact factor: 6.116

4.  Silica-Based Infiltrations for Enhanced Zirconia-Resin Interface Toughness.

Authors:  N C Ramos; M R Kaizer; T M B Campos; J Kim; Y Zhang; R M Melo
Journal:  J Dent Res       Date:  2019-02-14       Impact factor: 6.116

5.  Sliding contact fracture of dental ceramics: Principles and validation.

Authors:  Linlin Ren; Yu Zhang
Journal:  Acta Biomater       Date:  2014-03-12       Impact factor: 8.947

6.  Graded Ultra-Translucent Zirconia (5Y-PSZ) for Strength and Functionalities.

Authors:  L Mao; M R Kaizer; M Zhao; B Guo; Y F Song; Y Zhang
Journal:  J Dent Res       Date:  2018-04-25       Impact factor: 6.116

7.  The progressive wear and abrasiveness of novel graded glass/zirconia materials relative to their dental ceramic counterparts.

Authors:  Marina R Kaizer; Rafael R Moraes; Sergio S Cava; Yu Zhang
Journal:  Dent Mater       Date:  2019-03-01       Impact factor: 5.304

8.  Load-bearing capacity of lithium disilicate and ultra-translucent zirconias.

Authors:  Jing Yan; Marina R Kaizer; Yu Zhang
Journal:  J Mech Behav Biomed Mater       Date:  2018-08-21

9.  Load-bearing properties of minimal-invasive monolithic lithium disilicate and zirconia occlusal onlays: finite element and theoretical analyses.

Authors:  Li Ma; Petra C Guess; Yu Zhang
Journal:  Dent Mater       Date:  2013-05-15       Impact factor: 5.304

10.  On the interfacial fracture resistance of resin-bonded zirconia and glass-infiltrated graded zirconia.

Authors:  Herzl Chai; Marina Kaizer; Asima Chughtai; Hui Tong; Carina Tanaka; Yu Zhang
Journal:  Dent Mater       Date:  2015-09-11       Impact factor: 5.304

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.