HIP zirconia fixed partial dentures--clinical results after 3 years of clinical service.

Daniel Edelhoff1, Beuer Florian, Weber Florian, Christine Johnen.   

Abstract

OBJECTIVE: To evaluate prospectively the clinical performance of 3- to 6-unit zirconia fixed partial dentures (FPDs) after more than 3 years of clinical service. METHOD AND MATERIALS: Since August 2002, 22 conventional all-ceramic FPDs have been inserted in 18 patients. Nineteen of the FPDs were placed with a resin-reinforced glass-ionomer cement. The frameworks were manufactured by a universal CAD/CAM production system, milling the zirconia out of the densely sintered stage. The frameworks were designed as 3-unit (14), 4-unit (3), 5-unit (2), and 6-unit FPDs (3) for the anterior and posterior regions. A new synthetic sintering glass-ceramic was employed as the veneering material. In the follow-up examinations at baseline, 6, 12, 24, and 36 months, 21 FPDs were inspected predominantly for framework fractures and chipping of the veneering material. Besides these parameters, periodontal status, sensitivity of the abutment teeth, esthetic outcome, as well as the incidence of secondary caries, were evaluated.
RESULTS: After a mean clinical observation of over 39 months, no framework fracture occurred. However, chipping of the veneering material was reported in 2 cases.
CONCLUSION: All-ceramic FPDs based on zirconia frameworks exhibited satisfactory clinical performance.

Entities:  

Mesh:

Substances:

Year:  2008        PMID: 19057742

Source DB:  PubMed          Journal:  Quintessence Int        ISSN: 0033-6572            Impact factor:   1.677


  24 in total

1.  Shear bond strength between an indirect composite layering material and feldspathic porcelain-coated zirconia ceramics.

Authors:  Ryosuke Fushiki; Futoshi Komine; Markus B Blatz; Mai Koizuka; Kohei Taguchi; Hideo Matsumura
Journal:  Clin Oral Investig       Date:  2011-12-06       Impact factor: 3.573

2.  The effect of zirconia sintering temperature on flexural strength, grain size, and contrast ratio.

Authors:  Bogna Stawarczyk; Mutlu Ozcan; Lubica Hallmann; Andreas Ender; Albert Mehl; Christoph H F Hämmerlet
Journal:  Clin Oral Investig       Date:  2012-02-23       Impact factor: 3.573

3.  Overview: Damage resistance of graded ceramic restorative materials.

Authors:  Yu Zhang
Journal:  J Eur Ceram Soc       Date:  2012-08-01       Impact factor: 5.302

4.  Tooth-implant-supported posterior fixed dental prostheses with zirconia frameworks: 3-year clinical result.

Authors:  Florian Beuer; Caroline Sachs; Julian Groesser; Jan-Frederik Gueth; Michael Stimmelmayr
Journal:  Clin Oral Investig       Date:  2015-09-24       Impact factor: 3.573

5.  Sliding contact fatigue of graded zirconia with external esthetic glass.

Authors:  L Ren; M N Janal; Y Zhang
Journal:  J Dent Res       Date:  2011-06-10       Impact factor: 6.116

Review 6.  Performance of dental ceramics: challenges for improvements.

Authors:  E D Rekow; N R F A Silva; P G Coelho; Y Zhang; P Guess; V P Thompson
Journal:  J Dent Res       Date:  2011-01-11       Impact factor: 6.116

7.  Marginal and internal fit of posterior three-unit fixed zirconia dental prostheses fabricated with two different CAD/CAM systems and materials.

Authors:  Joana Schönberger; Kurt-Jürgen Erdelt; Daniel Bäumer; Florian Beuer
Journal:  Clin Oral Investig       Date:  2017-02-04       Impact factor: 3.573

8.  Strength of zirconia fixed partial dentures: review of the literature.

Authors:  M Gargari; F Gloria; A Cappello; L Ottria
Journal:  Oral Implantol (Rome)       Date:  2011-01-23

Review 9.  New Knowledge about Zirconium-Ceramic as a Structural Material in Fixed Prosthodontics.

Authors:  Davor Špehar; Marko Jakovac
Journal:  Acta Stomatol Croat       Date:  2015-06

10.  Ten-year survival and chipping rates and clinical quality grading of zirconia-based fixed dental prostheses.

Authors:  Maren Teichmann; Anna Lena Wienert; Marcia Rückbeil; Volker Weber; Stefan Wolfart; Daniel Edelhoff
Journal:  Clin Oral Investig       Date:  2018-03-08       Impact factor: 3.573

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.