A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics.

W Höland1, M Schweiger, M Frank, V Rheinberger.   

Abstract

The aim of this report is to analyze the microstructures of glass-ceramics of the IPS Empress 2 and IPS Empress systems by scanning electron microscopy. The main properties of the glass-ceramics were determined and compared to each other. The flexural strength of the pressed glass-ceramic (core material) was improved by a factor of more than three for IPS Empress 2 (lithium disilicate glass-ceramic) in comparison with IPS Empress (leucite glass-ceramic). For the fracture toughness, the K(IC) value was measured as 3.3 +/- 0.3 MPa. m(0.5) for IPS Empress 2 and 1.3 +/- 0.1 MPa. m(0.5) for IPS Empress. Abrasion behavior, chemical durability, and optical properties such as translucency of all glass-ceramics fulfill the dental standards. The authors concluded that IPS Empress 2 can be used to fabricate 3-unit bridges up to the second premolar. Copyright 2000 John Wiley & Sons, Inc.

Entities:  

Mesh:

Substances:

Year:  2000        PMID: 10898870     DOI: 10.1002/1097-4636(2000)53:4<297::aid-jbm3>3.0.co;2-g

Source DB:  PubMed          Journal:  J Biomed Mater Res        ISSN: 0021-9304


  36 in total

1.  Chipping fracture resistance of dental CAD/CAM restorative materials: part I--procedures and results.

Authors:  G D Quinn; A A Giuseppetti; K H Hoffman
Journal:  Dent Mater       Date:  2014-03-29       Impact factor: 5.304

2.  Influence of thermocycling on the optical properties of laboratory resin composites and an all-ceramic material.

Authors:  Seung-Hun Lee; Yong-Keun Lee; Bum-Soon Lim
Journal:  J Mater Sci Mater Med       Date:  2004-11       Impact factor: 3.896

3.  Finite element analysis to compare stress distribution of connector of lithia disilicate-reinforced glass-ceramic and zirconia-based fixed partial denture.

Authors:  Jie Lin; Akikazu Shinya; Harunori Gomi; Akiyoshi Shinya
Journal:  Odontology       Date:  2011-06-21       Impact factor: 2.634

Review 4.  Ocular prosthesis incorporating IPS e-max press scleral veneer and a literature review on non-integrated ocular prosthesis.

Authors:  Godwin Clovis Da Costa; Meena Ajay Aras; Paul Chalakkal; Michelle Clovis Da Costa
Journal:  Int J Ophthalmol       Date:  2017-01-18       Impact factor: 1.779

5.  Three years in vivo wear: core-ceramic, veneers, and enamel antagonists.

Authors:  Josephine F Esquivel-Upshaw; William F Rose; Allyson A Barrett; Erica R Oliveira; Mark C K Yang; Arthur E Clark; Kenneth J Anusavice
Journal:  Dent Mater       Date:  2012-03-10       Impact factor: 5.304

6.  Microhardness evaluations of CAD/CAM ceramics irradiated with CO2 or Nd:YAP laser.

Authors:  Ahmed El Gamal; Jean Paul Rocca; Carlo Fornaini; Etienne Medioni; Nathalie Brulat-Bouchard
Journal:  Laser Ther       Date:  2017-03-31

7.  Fracture surface analysis of clinically failed fixed partial dentures.

Authors:  B Taskonak; J J Mecholsky; K J Anusavice
Journal:  J Dent Res       Date:  2006-03       Impact factor: 6.116

8.  The effect of CO2 and Nd:YAP lasers on CAD/CAM Ceramics: SEM, EDS and thermal studies.

Authors:  Ahmed El Gamal; Carlo Fornaini; Jean Paul Rocca; Omid H Muhammad; Etienne Medioni; Annamaria Cucinotta; Nathalie Brulat-Bouchard
Journal:  Laser Ther       Date:  2016-03-31

9.  Three-unit CAD/CAM-generated lithium disilicate FDPs after a mean observation time of 46 months.

Authors:  Sven Reich; Lutz Endres; Claudia Weber; Klaus Wiedhahn; Peter Neumann; Oliver Schneider; Nicole Rafai; Stefan Wolfart
Journal:  Clin Oral Investig       Date:  2014-02-04       Impact factor: 3.573

10.  Chair-side generated posterior lithium disilicate crowns after 4 years.

Authors:  Sven Reich; Oliver Schierz
Journal:  Clin Oral Investig       Date:  2012-11-08       Impact factor: 3.573

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.