Effect of surface coatings on flexural properties of glass ionomers.

M Miyazaki1, B K Moore, H Onose.   

Abstract

The purpose of this study was to investigate the change in flexural strength and fracture toughness of light-cured glass ionomer cements after long-term immersion in water, and to investigate the effect of surface coatings on their properties. 2 resin-modified and 1 conventional glass ionomer cements were employed. For the flexural strength, a 25 x 2 x 2 mm stainless steel mold was used. For the fracture toughness (KtC), single edge notch specimens with dimensions 25 x 2.5 x 5 mm and a 0.5 mm notch (a/W = 0.5) were prepared in a stainless steel mold. Specimens were subjected to the 3 point bending at 0.5 mm/min after storage in 37 degrees C water for the periods of 1 h, 24 h, 1 wk, 1 month, and 6 months. The glass ionomer cements tended to exhibit an increase in mechanical properties over the 24-h period and then to maintain a constant strength. The surface protection of the resin-modified glass ionomer cement has some effect on the mechanical properties during early setting reactions, and it is desirable that the cement should be protected from direct water contact for at least 1 h after cement mixing.

Entities:  

Mesh:

Substances:

Year:  1996        PMID: 9021332     DOI: 10.1111/j.1600-0722.1996.tb00148.x

Source DB:  PubMed          Journal:  Eur J Oral Sci        ISSN: 0909-8836            Impact factor:   2.612


  6 in total

1.  The effect of resin coating on the shear punch strength of restorative glass ionomer cements.

Authors:  Raphael Pilo; Ariel Ben-Amar; Anna Barnea; Yaron Blasbalg; Shifra Levartovsky
Journal:  Clin Oral Investig       Date:  2016-06-04       Impact factor: 3.573

2.  Investigation of water sorption and aluminum releases from high viscosity and resin modified glass ionomer.

Authors:  Numan Aydın; Serpil Karaoğlanoğlu; Elif Aybala-Oktay; Serdar Çetinkaya; Onur Erdem
Journal:  J Clin Exp Dent       Date:  2020-09-01

3.  In vitro abrasion of resin-coated highly viscous glass ionomer cements: a confocal laser scanning microscopy study.

Authors:  Özgur Kanik; L Sebnem Turkun; Walter Dasch
Journal:  Clin Oral Investig       Date:  2016-04-13       Impact factor: 3.573

4.  Clinical performance during 48 months of two current glass ionomer restorative systems with coatings: a randomized clinical trial in the field.

Authors:  Thomas Klinke; Amro Daboul; Anita Turek; Roland Frankenberger; Reinhard Hickel; Reiner Biffar
Journal:  Trials       Date:  2016-05-08       Impact factor: 2.279

5.  Long-Term Water Balance Evaluation in Glass Ionomer Restorative Materials.

Authors:  Howard Roberts; David Berzins; John Nicholson
Journal:  Materials (Basel)       Date:  2022-01-21       Impact factor: 3.623

6.  The Effect of Nanofilled Resin-Base Coating on the Mechanical and Physical Properties of Resin Composites.

Authors:  Negar Moghaddasi; Maryam Tavallali; Dana Jafarpour; Reihaneh Ferooz; Rafat Bagheri
Journal:  Eur J Dent       Date:  2020-10-27
  6 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.