Literature DB >> 8603209

A review of methods used to reinforce polymethyl methacrylate resin.

P K Vallittu1.   

Abstract

Various methods to reinforce acrylic denture base material have been used to repair fractures in complete dentures. Metal wires and plates have been tested as reinforcement of polymethyl methacrylate (PMMA) resin. The contributions of the studies conducted on this biphase composite system are discussed in this review article. The literature has reported that even thin metal wires incorporated into the PMMA matrix increased the transverse strength of the PMMA construction. Metal mesh inserted into PMMA resin had negligible effects on the transverse strength of the restoration. macroscopic retention of the metal strengtheners to the PMMA had only a minor effect on the strength in contrast to microscopic retention, which showed a more marked effect. Chemical bonding between the PMMA and metal reinforcer enhanced the strength of the prosthesis with some exceptions.

Entities:  

Mesh:

Substances:

Year:  1995        PMID: 8603209     DOI: 10.1111/j.1532-849x.1995.tb00338.x

Source DB:  PubMed          Journal:  J Prosthodont        ISSN: 1059-941X            Impact factor:   2.752


  20 in total

1.  Evaluation of flexural strength of resin interim restorations impregnated with various types of silane treated and untreated glass fibres.

Authors:  K S Naveen; J P Singh; M Viswambaran; R K Dhiman
Journal:  Med J Armed Forces India       Date:  2012-09-14

2.  The effect of incorporation, orientation and silane treatment of glass fibers on the fracture resistance of interim fixed partial dentures.

Authors:  Gupta Basant; Y G Reddy
Journal:  J Indian Prosthodont Soc       Date:  2011-04-17

3.  A novel endoscopic fluorescent clip for the localization of gastrointestinal tumors.

Authors:  Yongdoo Choi; Kwang Gi Kim; Joa Kyum Kim; Kyoung Won Nam; Hyun Ho Kim; Dae Kyung Sohn
Journal:  Surg Endosc       Date:  2011-02-07       Impact factor: 4.584

4.  The effect of glass and polyethylene fiber reinforcement on flexural strength of provisional restorative resins: an in vitro study.

Authors:  Parthasarathy Natarajan; C Thulasingam
Journal:  J Indian Prosthodont Soc       Date:  2012-07-14

5.  An evaluation of fracture resistance of interim fixed partial denture fabricated using polymethylmethacrylate and reinforced by different fibres for its optimal placement: an in vitro study.

Authors:  M Viswambaran; Anita Kapri; Dsj D'Souza; Manjit Kumar
Journal:  Med J Armed Forces India       Date:  2011-10-22

6.  Effect of nanosilver on thermal and mechanical properties of acrylic base complete dentures.

Authors:  Fahimeh Hamedi-Rad; Tahereh Ghaffari; Farzad Rezaii; Ali Ramazani
Journal:  J Dent (Tehran)       Date:  2014-09-30

7.  Comparison of fiber reinforcement placed at different locations of pontic in interim fixed partial denture to prevent fracture: An in vitro study.

Authors:  Surg Cdr Anita Kapri
Journal:  J Indian Prosthodont Soc       Date:  2015 Apr-Jun

8.  A comparative study to check fracture strength of provisional fixed partial dentures made of autopolymerizing polymethylmethacrylate resin reinforced with different materials: An in vitro study.

Authors:  Parikshit Gupt; Archana Nagpal; Rupandeep Kaur Samra; Ramit Verma; Jasjeet Kaur; Surbhi Abrol
Journal:  J Indian Prosthodont Soc       Date:  2017 Jul-Sep

9.  Effect of Water Storage on the Flexural Strength of Heat-cured Denture Base Resin Reinforced with Stick (s) Glass Fibers.

Authors:  Ankit Galav; Suryakant C Deogade; Sneha Mantri; K Sumathi; Sneha Galav
Journal:  Contemp Clin Dent       Date:  2017 Apr-Jun

10.  Effects of incorporation of 2.5 and 5 wt% TiO2 nanotubes on fracture toughness, flexural strength, and microhardness of denture base poly methyl methacrylate (PMMA).

Authors:  Sahar Abdulrazzaq Naji; Marjan Behroozibakhsh; Tahereh Sadat Jafarzadeh Kashi; Hossein Eslami; Reza Masaeli; Hosseinali Mahgoli; Mohammadreza Tahriri; Mehrsima Ghavvami Lahiji; Vahid Rakhshan
Journal:  J Adv Prosthodont       Date:  2018-04-18       Impact factor: 1.904

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.