Effect of different dental ceramic systems on the wear of human enamel: An in vitro study.

Roya Zandparsa1, Rabie M El Huni2, Hiroshi Hirayama3, Marc I Johnson4.   

Abstract

STATEMENT OF PROBLEM: The wear of tooth structure opposing different advanced dental ceramic systems requires investigation.
PURPOSE: The purpose of this in vitro study was to compare the wear of advanced ceramic systems against human enamel antagonists.
MATERIAL AND METHODS: Four ceramic systems (IPS e.max Press, IPS e.max CAD, Noritake Super Porcelain EX-3, and LAVA Plus Zirconia) and 1 control group containing human enamel specimens were used in this study (n = 12). All specimens were fabricated as disks 11 mm in diameter and 3 mm thick. The mesiopalatal cusps of the maxillary third molars were prepared to serve as the enamel styluses. All specimens were embedded individually in 25 mm(3) autopolymerizing acrylic resin blocks. Wear was measured with a cyclic loading machine and a newly designed wear simulator. All enamel styluses (cusps) were scanned using the Activity 880 digital scanner (SmartOptics). Data from the base line and follow-up scans were collected and compared with Qualify 2012 3-dimensional (3D) and 2D digital inspection software (Geomagic), which aligned the models and detected the geometric changes and the wear caused by the antagonist specimen. One-way ANOVA was used to analyze the collected data.
RESULTS: After 125,000 bidirectional loading cycles, the mean loss of opposing enamel volume for the enamel disks in the control group was 37.08 μm(3), the lowest mean value for IPS e.max Press system was 39.75 μm(3); 40.58 μm(3) for IPS e.max CAD; 45.08 μm(3) for Noritake Super Porcelain EX-3 system; and 48.66 μm(3) for the Lava Plus Zirconia system. No statically significant differences were found among the groups in opposing enamel volume loss (P=.225) or opposing enamel height loss (P=.149). In terms of opposing enamel height loss, Lava Plus Zirconia system showed the lowest mean value of 27.5 μm. The mean value for the IPS e.max CAD system was 27.91 μm; 29.08 μm for the control enamel; 33.25 μm for the IPS e.max Press system; and 34.75 μm for the Noritake Super Porcelain EX-3 system.
CONCLUSIONS: Within the limitations of this in vitro study, no differences were found in the linear and volumetric reduction of enamel cusps abraded against enamel disks and all other ceramic specimens. All ceramic systems exhibited high durability and were wear-friendly to opposing enamel.
Copyright © 2016 Editorial Council for the Journal of Prosthetic Dentistry. Published by Elsevier Inc. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2015        PMID: 26548885     DOI: 10.1016/j.prosdent.2015.09.005

Source DB:  PubMed          Journal:  J Prosthet Dent        ISSN: 0022-3913            Impact factor:   3.426


  10 in total

1.  The flexural strength of CAD/CAM polymer crowns and the effect of artificial ageing on the fracture resistance of CAD/CAM polymer and ceramic single crowns.

Authors:  Anna Winter; Axel Schurig; Engelke Rasche; Franziska Rösner; Lisa Kanus; Marc Schmitter
Journal:  J Mater Sci Mater Med       Date:  2019-12-23       Impact factor: 3.896

2.  Randomized clinical study of wear of enamel antagonists against polished monolithic zirconia crowns.

Authors:  J F Esquivel-Upshaw; M J Kim; S M Hsu; N Abdulhameed; R Jenkins; D Neal; F Ren; A E Clark
Journal:  J Dent       Date:  2017-10-16       Impact factor: 4.379

3.  Effect of framework type on survival probability of implant-supported temporary crowns: An in vitro study.

Authors:  Vinícius-Anéas Rodrigues; Amanda-Maria-de Oliveira Dal Piva; Claudio-Akira Yamaguchi; Alexandre-Luiz-Souto Borges; Marcio-Katsuyoshi Mukai; João-Paulo-Mendes Tribst
Journal:  J Clin Exp Dent       Date:  2020-05-01

4.  Two-body wear behavior of human enamel versus monolithic zirconia, lithium disilicate, ceramometal and composite resin.

Authors:  Syed Rashid Habib; Abdulaziz Alotaibi; Nawaf Al Hazza; Yasser Allam; Mohammad AlGhazi
Journal:  J Adv Prosthodont       Date:  2019-02-26       Impact factor: 1.904

5.  Wear Characteristics of Dental Ceramic CAD/CAM Materials Opposing Various Dental Composite Resins.

Authors:  Bora Gwon; Eun-Bin Bae; Jin-Ju Lee; Won-Tak Cho; Hyun-Young Bae; Jae-Won Choi; Jung-Bo Huh
Journal:  Materials (Basel)       Date:  2019-06-06       Impact factor: 3.623

Review 6.  In Vitro Simulation and In Vivo Assessment of Tooth Wear: A Meta-Analysis of In Vitro and Clinical Research.

Authors:  Despina Koletsi; Anna Iliadi; Theodore Eliades; George Eliades
Journal:  Materials (Basel)       Date:  2019-10-31       Impact factor: 3.623

Review 7.  Wear in Antagonist Teeth Produced by Monolithic Zirconia Crowns: A Systematic Review and Meta-Analysis.

Authors:  María Fernanda Solá-Ruíz; Alejandra Baima-Moscardó; Eduardo Selva-Otaolaurruchi; José María Montiel-Company; Rubén Agustín-Panadero; Carla Fons-Badal; Lucía Fernández-Estevan
Journal:  J Clin Med       Date:  2020-04-02       Impact factor: 4.241

8.  Influence of zirconia and lithium disilicate tooth- or implant-supported crowns on wear of antagonistic and adjacent teeth.

Authors:  Martin Rosentritt; Frederik Schumann; Stephanie Krifka; Verena Preis
Journal:  J Adv Prosthodont       Date:  2020-02-20       Impact factor: 1.904

9.  In-vivo-wear in composite and ceramic full mouth rehabilitations over 3 years.

Authors:  Gintare Burian; Kurt Erdelt; Josef Schweiger; Christine Keul; Daniel Edelhoff; Jan-Frederik Güth
Journal:  Sci Rep       Date:  2021-07-07       Impact factor: 4.379

10.  Comparative evaluation of natural enamel wear against polished yitrium tetragonal zirconia and polished lithium disilicate - An in vivo study.

Authors:  Girish S Nazirkar; Swati Vijay Patil; Priyanka P Shelke; Preetam Mahagaonkar
Journal:  J Indian Prosthodont Soc       Date:  2020-01-27
  10 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.