Literature DB >> 22178651

Designing functionally graded materials with superior load-bearing properties.

Yu Zhang1, Ming-Jie Sun, Denzil Zhang.   

Abstract

Ceramic prostheses often fail from fracture and wear. We hypothesize that these failures may be substantially mitigated by an appropriate grading of elastic modulus at the ceramic surface. In this study, we elucidate the effect of elastic modulus profile on the flexural damage resistance of functionally graded materials (FGMs), providing theoretical guidelines for designing FGMs with superior load-bearing property. The Young's modulus of the graded structure is assumed to vary in a power-law relation with a scaling exponent n; this is in accordance with experimental observations from our laboratory and elsewhere. Based on the theory for bending of graded beams, we examine the effect of n value and bulk-to-surface modulus ratio (E(b)/E(s)) on stress distribution through the graded layer. Theory predicts that a low exponent (0.15<n<0.5), coupled with a relatively small modulus ratio (3<E(b)/E(s)<6), is most desirable for reducing the maximum stress and transferring it into the interior, while keeping the surface stress low. Experimentally, we demonstrate that elastically graded materials with various n values and E(b)/E(s) ratios can be fabricated by infiltrating alumina and zirconia with a low-modulus glass. Flexural tests show that graded alumina and zirconia with suitable values of these parameters exhibit superior load-bearing capacity, 20-50% higher than their homogeneous counterparts. Improving load-bearing capacity of ceramic materials could have broad impacts on biomedical, civil, structural, and an array of other engineering applications.
Copyright © 2011 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2011        PMID: 22178651      PMCID: PMC3272119          DOI: 10.1016/j.actbio.2011.11.033

Source DB:  PubMed          Journal:  Acta Biomater        ISSN: 1742-7061            Impact factor:   8.947


  26 in total

Review 1.  Clinically relevant approach to failure testing of all-ceramic restorations.

Authors:  J R Kelly
Journal:  J Prosthet Dent       Date:  1999-06       Impact factor: 3.426

2.  The Bisurface total knee replacement: a unique design for flexion. Four-to-nine-year follow-up study.

Authors:  M Akagi; T Nakamura; Y Matsusue; T Ueo; K Nishijyo; E Ohnishi
Journal:  J Bone Joint Surg Am       Date:  2000-11       Impact factor: 5.284

3.  Long-term strength of ceramics for biomedical applications.

Authors:  Yu Zhang; Brian Lawn
Journal:  J Biomed Mater Res B Appl Biomater       Date:  2004-05-15       Impact factor: 3.368

Review 4.  Dental ceramics: current thinking and trends.

Authors:  J Robert Kelly
Journal:  Dent Clin North Am       Date:  2004-04

5.  Bioinspired design of dental multilayers.

Authors:  M Huang; R Wang; V Thompson; D Rekow; W O Soboyejo
Journal:  J Mater Sci Mater Med       Date:  2007-01       Impact factor: 3.896

Review 6.  Hard bearing surfaces in total hip arthroplasty.

Authors:  L M Jazrawi; F J Kummer; P E Di Cesare
Journal:  Am J Orthop (Belle Mead NJ)       Date:  1998-04

7.  Improving fatigue damage resistance of alumina through surface grading.

Authors:  L Ren; L Liu; S Bhowmick; Y B Gerbig; M N Janal; V P Thompson; Y Zhang
Journal:  J Dent Res       Date:  2011-05-09       Impact factor: 6.116

8.  Graded zirconia glass for resistance to veneer fracture.

Authors:  Y Zhang; J W Kim
Journal:  J Dent Res       Date:  2010-07-22       Impact factor: 6.116

Review 9.  Review on ceramic-on-ceramic total hip arthroplasty.

Authors:  S Mehmood; Riyaz H Jinnah; Hemant Pandit
Journal:  J Surg Orthop Adv       Date:  2008

Review 10.  Zirconia as a ceramic biomaterial.

Authors:  C Piconi; G Maccauro
Journal:  Biomaterials       Date:  1999-01       Impact factor: 12.479

View more
  17 in total

1.  Overview: Damage resistance of graded ceramic restorative materials.

Authors:  Yu Zhang
Journal:  J Eur Ceram Soc       Date:  2012-08-01       Impact factor: 5.302

2.  Using glass-graded zirconia to increase delamination growth resistance in porcelain/zirconia dental structures.

Authors:  Herzl Chai; Adam J Mieleszko; Stephen J Chu; Yu Zhang
Journal:  Dent Mater       Date:  2017-11-26       Impact factor: 5.304

3.  On the interfacial fracture of porcelain/zirconia and graded zirconia dental structures.

Authors:  Herzl Chai; James J-W Lee; Adam J Mieleszko; Stephen J Chu; Yu Zhang
Journal:  Acta Biomater       Date:  2014-04-24       Impact factor: 8.947

Review 4.  Zirconia surface modifications for implant dentistry.

Authors:  Fernanda H Schünemann; María E Galárraga-Vinueza; Ricardo Magini; Márcio Fredel; Filipe Silva; Júlio C M Souza; Yu Zhang; Bruno Henriques
Journal:  Mater Sci Eng C Mater Biol Appl       Date:  2019-01-16       Impact factor: 7.328

5.  Sliding contact fracture of dental ceramics: Principles and validation.

Authors:  Linlin Ren; Yu Zhang
Journal:  Acta Biomater       Date:  2014-03-12       Impact factor: 8.947

6.  Effects of cementation surface modifications on fracture resistance of zirconia.

Authors:  Ramanathan Srikanth; Tomaz Kosmac; Alvaro Della Bona; Ling Yin; Yu Zhang
Journal:  Dent Mater       Date:  2015-02-14       Impact factor: 5.304

7.  Influence of interlayer design on residual thermal stresses in trilayered and graded all-ceramic restorations.

Authors:  Bruno Henriques; Douglas Fabris; Júlio C M Souza; Filipe S Silva; Joana Mesquita-Guimarães; Yu Zhang; Márcio Fredel
Journal:  Mater Sci Eng C Mater Biol Appl       Date:  2016-11-25       Impact factor: 7.328

8.  The bending stress distribution in bilayered and graded zirconia-based dental ceramics.

Authors:  Douglas Fabris; Júlio C M Souza; Filipe S Silva; Márcio Fredel; Joana Mesquita-Guimarães; Yu Zhang; Bruno Henriques
Journal:  Ceram Int       Date:  2016-04-01       Impact factor: 4.527

9.  THERMAL RESIDUAL STRESSES IN BILAYERED, TRILAYERED AND GRADED DENTAL CERAMICS.

Authors:  Douglas Fabris; Júlio C M Souza; Filipe S Silva; Márcio Fredel; Joana Mesquita-Guimarães; Yu Zhang; Bruno Henriques
Journal:  Ceram Int       Date:  2016-12-01       Impact factor: 4.527

10.  On the interfacial fracture resistance of resin-bonded zirconia and glass-infiltrated graded zirconia.

Authors:  Herzl Chai; Marina Kaizer; Asima Chughtai; Hui Tong; Carina Tanaka; Yu Zhang
Journal:  Dent Mater       Date:  2015-09-11       Impact factor: 5.304

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.