Quantitative measurement of tooth and ceramic wear: in vivo study.

Maged K Etman1, Mark Woolford, Stephen Dunne.   

Abstract

PURPOSE: The aim of this study was to quantitatively measure tooth and ceramic wear over a 2-year period using a novel superimposition technique. Three ceramic systems--experimental hot-pressed ceramic (EC), Procera AllCeram (PA), and metal-ceramic--were used.
MATERIALS AND METHODS: A total of 90 posterior crowns in 48 patients were randomized into 3 groups, and impressions were made at baseline and at 6-month intervals for 2 years. Clinical images were taken after using a dye to highlight surface changes. The impressions were digitized and modeled as superimposable 3-dimensional colored surface images. The depth of wear at the occlusal contact areas was quantitatively measured at 6, 12, 18, and 24 months.
RESULTS: The quantitative evaluation showed more wear in Procera AllCeram at the occlusal contact areas, whereas the experimental and metal-ceramic systems showed less wear. There was a significant difference in the amount of enamel worn between all types of restorations (P < .05). There was a statistically significant difference (P < .05) in the mean depth of wear between all systems.
CONCLUSIONS: The metal-ceramic and experimental systems showed less change, indicating improved wear resistance compared with Procera AllCeram. In addition, enamel opposing metal-ceramic and experimental crowns showed less wear compared to enamel opposed by Procera AIICeram crowns.

Entities:  

Mesh:

Substances:

Year:  2008        PMID: 18548965

Source DB:  PubMed          Journal:  Int J Prosthodont        ISSN: 0893-2174            Impact factor:   1.681


  17 in total

1.  Two-body wear of dental porcelain and substructure oxide ceramics.

Authors:  Martin Rosentritt; Verena Preis; Michael Behr; Sebastian Hahnel; Gerhard Handel; Carola Kolbeck
Journal:  Clin Oral Investig       Date:  2011-07-08       Impact factor: 3.573

Review 2.  Ocular prosthesis incorporating IPS e-max press scleral veneer and a literature review on non-integrated ocular prosthesis.

Authors:  Godwin Clovis Da Costa; Meena Ajay Aras; Paul Chalakkal; Michelle Clovis Da Costa
Journal:  Int J Ophthalmol       Date:  2017-01-18       Impact factor: 1.779

3.  Effect of finishing/polishing techniques and low temperature degradation on the surface topography, phase transformation and flexural strength of ultra-translucent ZrO2 ceramic.

Authors:  Taciana Emília Leite Vila-Nova; Isabelle Helena Gurgel de Carvalho; Dayanne Monielle Duarte Moura; André Ulisses Dantas Batista; Yu Zhang; Carlos Alberto Paskocimas; Marco Antonio Bottino; Rodrigo Othávio de Assunção E Souza
Journal:  Dent Mater       Date:  2020-01-31       Impact factor: 5.304

4.  Antagonist wear of monolithic zirconia crowns after 2 years.

Authors:  Ulrich Lohbauer; Sven Reich
Journal:  Clin Oral Investig       Date:  2016-06-09       Impact factor: 3.573

5.  Speed sintering translucent zirconia for chairside one-visit dental restorations: Optical, mechanical, and wear characteristics.

Authors:  Marina R Kaizer; Petra C Gierthmuehlen; Mateus Bf Dos Santos; Sergio S Cava; Yu Zhang
Journal:  Ceram Int       Date:  2017-05-19       Impact factor: 4.527

6.  Comprehensive analysis of laserscanner validity used for measurement of wear.

Authors:  Shu-Min Hsu; Fan Ren; Nader Abdulhameed; Mijin Kim; Dan Neal; Josephine Esquivel-Upshaw
Journal:  J Oral Rehabil       Date:  2019-03-14       Impact factor: 3.837

7.  The progressive wear and abrasiveness of novel graded glass/zirconia materials relative to their dental ceramic counterparts.

Authors:  Marina R Kaizer; Rafael R Moraes; Sergio S Cava; Yu Zhang
Journal:  Dent Mater       Date:  2019-03-01       Impact factor: 5.304

8.  Three years in vivo wear: core-ceramic, veneers, and enamel antagonists.

Authors:  Josephine F Esquivel-Upshaw; William F Rose; Allyson A Barrett; Erica R Oliveira; Mark C K Yang; Arthur E Clark; Kenneth J Anusavice
Journal:  Dent Mater       Date:  2012-03-10       Impact factor: 5.304

9.  Effects of Different Polishing Systems on Surface Roughness and Crystal Structure of Zirconia.

Authors:  Cheng Chen; Xiaohua Zeng
Journal:  Appl Bionics Biomech       Date:  2022-05-09       Impact factor: 1.781

Review 10.  Tooth wear against ceramic crowns in posterior region: a systematic literature review.

Authors:  Rim Hmaidouch; Paul Weigl
Journal:  Int J Oral Sci       Date:  2013-10-18       Impact factor: 6.344

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.