Literature DB >> 16199410

A comparison of tungsten-quartz-halogen, plasma arc and light-emitting diode light sources for the polymerization of an orthodontic adhesive.

Bikram S Thind1, David R Stirrups, Charles H Lloyd.   

Abstract

This study investigated whether there were differences between the debond stress and adhesive remnant index (ARI) of an adhesive cured with three different orthodontic light sources. Sixty sound premolar teeth were divided into three groups of 20. A standard pre-adjusted edgewise premolar bracket (Victory Series) was bonded to each tooth using a light-cured orthodontic adhesive, Transbond X. Group 1 (control) specimens were cured with an Ortholux XT (tungsten-quartz-halogen bulb) light for 20 seconds, group 2 with an Ortho lite (plasma arc) for 6 seconds and group 3 with an Ortholux LED light-emitting diode for 10 seconds. The specimens were debonded 24 hours later using a universal mechanical testing machine, operating at a crosshead speed of 0.5 mm minute(-1). The Weibull modulus and a Logrank test showed no statistically significant differences between the three groups for debond stress. The ARI was assessed at x10 magnification. The ARI scores for group 2 were significantly different (P < 0.01) from those of groups 1 and 3 (between which there was no significant difference). For group 2 there was a greater tendency for failure to occur at the adhesive/tooth interface than for the other two groups. There appears to be no reason why any of the three types of light source cannot be used in orthodontics. Polymerization, as effective as that produced by conventional bulb light sources, was obtained with the short exposure times recommended for the plasma arc or light-emitting diode sources.

Entities:  

Mesh:

Substances:

Year:  2005        PMID: 16199410     DOI: 10.1093/ejo/cji076

Source DB:  PubMed          Journal:  Eur J Orthod        ISSN: 0141-5387            Impact factor:   3.075


  8 in total

1.  Effects of reducing light-curing time of a high-power LED device on shear bond strength of brackets.

Authors:  Layene Figueiredo Almeida; Lidia Parsekian Martins; Renato Parsekian Martins
Journal:  J Orofac Orthop       Date:  2018-07-31       Impact factor: 1.938

2.  Self-etch adhesives for the bonding of orthodontic brackets: faster, stronger, safer?

Authors:  Timea Lamper; Nicoleta Ilie; Karin C Huth; Ingrid Rudzki; Andrea Wichelhaus; Ekaterini Paschos
Journal:  Clin Oral Investig       Date:  2013-02-14       Impact factor: 3.573

3.  Influence of enamel conditioning on the shear bond strength of different adhesives.

Authors:  Lorenz Brauchli; Teodoro Muscillo; Markus Steineck; Andrea Wichelhaus
Journal:  J Orofac Orthop       Date:  2010-11-17       Impact factor: 1.938

4.  Effect of short curing times with a high-intensity light-emitting diode or high-power halogen on shear bond strength of metal brackets before and after thermocycling.

Authors:  Erion Cerekja; Banu Cakirer
Journal:  Angle Orthod       Date:  2011-01-24       Impact factor: 2.079

5.  Shear Bond Strength of Orthodontic Brackets Cured with Different Light Sources under Thermocycling.

Authors:  Oral Sokucu; Seyda Herguner Siso; Firat Ozturk; Ruhi Nalcaci
Journal:  Eur J Dent       Date:  2010-07

6.  Effect of Dental Chair Light on Enamel Bonding of Orthodontic Brackets Using Light Cure Based Adhesive System: An In-Vitro Study.

Authors:  Anil Tiwari; Tarulatha Shyagali; Sarvraj Kohli; Rishi Joshi; Abhishek Gupta; Rana Tiwari
Journal:  Acta Inform Med       Date:  2016-11-01

7.  Comparison of Bond Strength of Metal and Ceramic Brackets Bonded with Conventional and High-Power LED Light Curing Units.

Authors:  Javad Chalipa; Yasamin Farajzadeh Jalali; Fatemeh Gorjizadeh; Pedram Baghaeian; Mohammad Hashem Hoseini; Omid Mortezai
Journal:  J Dent (Tehran)       Date:  2016-11

8.  Shear bond strength of a bracket-bonding system cured with a light-emitting diode or halogen-based light-curing unit at various polymerization times.

Authors:  Sanjay Prasad Gupta; Basanta Kumar Shrestha
Journal:  Clin Cosmet Investig Dent       Date:  2018-04-10
  8 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.