Literature DB >> 12161462

Reliability and properties of ground Y-TZP-zirconia ceramics.

R G Luthardt1, M Holzhüter, O Sandkuhl, V Herold, J D Schnapp, E Kuhlisch, M Walter.   

Abstract

Yttria-stabilized zirconia ceramics is a high-performance material with excellent biocompatibility and mechanical properties, which suggest its suitability for posterior fixed partial dentures. The hypothesis under examination is that the strength and reliability of Y-TZP zirconia ceramics are affected by the inner surface grinding of crowns, and vary with the grinding parameter. Flexural strength, surface roughness, and fracture toughness were determined on samples machined by face and peripheral grinding with varied feed velocities and cutting depths. Results have been compared with those on lapped samples. Analysis of variance and Weibull parameter were used for statistical analysis. It was found that inner surface grinding significantly reduces the strength and reliability of Y-TZP zirconia compared with the lapped control sample. Co-analysis of flexural strength, Weibull parameter, and fracture toughness showed counteracting effects of surface compressive stress and grinding-introduced surface flaws. In conclusion, grinding of Y-TZP needs to be optimized to achieve the CAD/CAM manufacture of all-ceramic restorations with improved strength and reliability.

Entities:  

Mesh:

Substances:

Year:  2002        PMID: 12161462     DOI: 10.1177/154405910208100711

Source DB:  PubMed          Journal:  J Dent Res        ISSN: 0022-0345            Impact factor:   6.116


  48 in total

1.  Damage and reliability of Y-TZP after cementation surface treatment.

Authors:  P C Guess; Y Zhang; J-W Kim; E D Rekow; V P Thompson
Journal:  J Dent Res       Date:  2010-03-30       Impact factor: 6.116

Review 2.  Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?

Authors:  Jeffrey Y Thompson; Brian R Stoner; Jeffrey R Piascik; Robert Smith
Journal:  Dent Mater       Date:  2010-11-20       Impact factor: 5.304

3.  Parameters affecting retentive force of electroformed double-crown systems.

Authors:  Florian Beuer; Daniel Edelhoff; Wolfgang Gernet; Michael Naumann
Journal:  Clin Oral Investig       Date:  2009-04-03       Impact factor: 3.573

4.  Evaluation of the topographical surface changes and roughness of zirconia after different surface treatments.

Authors:  Meryem Gülce Subaşı; Özgür İnan
Journal:  Lasers Med Sci       Date:  2011-07-24       Impact factor: 3.161

5.  Influence of surface treatments and resin cement selection on bonding to zirconia.

Authors:  Meryem Gülce Subaşı; Özgür Inan
Journal:  Lasers Med Sci       Date:  2012-11-09       Impact factor: 3.161

6.  Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30 μm silica-coated alumina particles.

Authors:  Susanne S Scherrer; Maria Cattani-Lorente; Eric Vittecoq; François de Mestral; Jason A Griggs; H W Anselm Wiskott
Journal:  Dent Mater       Date:  2010-11-05       Impact factor: 5.304

7.  SEM evaluation of human gingival fibroblasts growth onto CAD/CAM zirconia and veneering ceramic for zirconia.

Authors:  Vincenzo Zizzari; Bruna Borelli; Marianna De Colli; Margherita Tumedei; Donato Di Iorio; Susi Zara; Roberto Sorrentino; Amelia Cataldi; Enrico Felice Gherlone; Fernando Zarone; Stefano Tetè
Journal:  Ann Stomatol (Roma)       Date:  2014-02-04

8.  Influence of finish line in the distribution of stress trough an all ceramic implant-supported crown.: A 3D Finite Element Analysis.

Authors:  G Sannino; F Gloria; L Ottria; A Barlattani
Journal:  Oral Implantol (Rome)       Date:  2010-03-04

9.  Effect of surface treatment on the micro-shear bond strength to zirconia.

Authors:  Esam Tashkandi
Journal:  Saudi Dent J       Date:  2009-10-29

10.  Effect of span length on the fit of zirconia framework fabricated using CAD/CAM system.

Authors:  Jeong-Yol Lee; Sang-Jin Choi; Min-Soo Kim; Ha-Young Kim; Young-Soo Kim; Sang-Wan Shin
Journal:  J Adv Prosthodont       Date:  2013-05-30       Impact factor: 1.904

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.