Fracture strength of all-ceramic lithium disilicate and porcelain-fused-to-metal bridges for molar replacement after dynamic loading.

Somsak Chitmongkolsuk1, Guido Heydecke, Christian Stappert, Joerg R Strub.   

Abstract

The replacement of missing posterior teeth using all-ceramic bridges remains a challenge. This study compares the fracture resistance of all-ceramic 3-unit bridges for the replacement of first molars to conventional porcelain-fused-to-metal bridges. Human premolars and molars were used to create two test groups and one control group of 16 specimens each. To simulate clinical parameters, the specimens were exposed to cyclic fatigue loading in an artificial mouth with simultaneous thermocycling. All samples were thereafter exposed to fracture strength testing. Porcelain-fused-to-metal bridges showed significantly higher fracture strengths than all-ceramic bridges. However, the fracture strength of the all-ceramic bridges was higher than peak physiological chewing forces.

Entities:  

Mesh:

Substances:

Year:  2002        PMID: 12051127

Source DB:  PubMed          Journal:  Eur J Prosthodont Restor Dent        ISSN: 0965-7452


  9 in total

1.  Surface roughness and Streptococcus mutans adhesion on surface sealant agent coupled interim crown materials after dynamic loading.

Authors:  Eda Eslemez Topcu; Onur Şahin; Ayşegül Köroğlu; Füsun Cömert; Burak Yilmaz
Journal:  BMC Oral Health       Date:  2022-07-19       Impact factor: 3.747

2.  Monolithic and bi-layer CAD/CAM lithium-disilicate versus metal-ceramic fixed dental prostheses: comparison of fracture loads and failure modes after fatigue.

Authors:  Stefan Schultheis; Joerg R Strub; Thomas A Gerds; Petra C Guess
Journal:  Clin Oral Investig       Date:  2012-09-22       Impact factor: 3.573

Review 3.  "Digitally Oriented Materials": Focus on Lithium Disilicate Ceramics.

Authors:  Fernando Zarone; Marco Ferrari; Francesco Guido Mangano; Renato Leone; Roberto Sorrentino
Journal:  Int J Dent       Date:  2016-08-18

4.  Fracture load and survival of anatomically representative monolithic lithium disilicate crowns with reduced tooth preparation and ceramic thickness.

Authors:  Noor A Nawafleh; Muhanad M Hatamleh; Andreas Öchsner; Florian Mack
Journal:  J Adv Prosthodont       Date:  2017-12-14       Impact factor: 1.904

5.  Fracture Strength of Three-Unit Implant Supported Fixed Partial Dentures with Excessive Crown Height Fabricated from Different Materials.

Authors:  Vahideh Nazari; Safoura Ghodsi; Marzieh Alikhasi; Majid Sahebi; Ahmad Reza Shamshiri
Journal:  J Dent (Tehran)       Date:  2016-11

6.  Effects of dynamic aging on the wear and fracture strength of monolithic zirconia restorations.

Authors:  Işıl Sarıkaya; Yeliz Hayran
Journal:  BMC Oral Health       Date:  2018-08-23       Impact factor: 2.757

Review 7.  Marginal and internal adaptation of lithium disilicate partial restorations: A systematic review and meta-analysis.

Authors:  Natália Almeida Bastos; Sandro Basso Bitencourt; Renan Figueiredo Carneiro; Brunna Mota Ferrairo; Samira Sandy Ferreira Strelhow; Daniela Micheline Dos Santos; Juliana Fraga Soares Bombonatti
Journal:  J Indian Prosthodont Soc       Date:  2020-10-08

8.  Flexural Strength of Vitreous Ceramics Based on Lithium Disilicate and Lithium Silicate Reinforced with Zirconia for CAD/CAM.

Authors:  Hazel P R Corado; Pedro H P M da Silveira; Vagner L Ortega; Guilherme G Ramos; Carlos N Elias
Journal:  Int J Biomater       Date:  2022-02-02

9.  Influence of preparation design on fracture resistance of different monolithic zirconia crowns: A comparative study.

Authors:  Meelad Basil Findakly; Haider Hasan Jasim
Journal:  J Adv Prosthodont       Date:  2019-12-18       Impact factor: 1.904

  9 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.