Literature DB >> 9758997

Effects of preparation and luting system on all-ceramic computer-generated crowns.

W H Mörmann1, A Bindl, H Lüthy, A Rathke.   

Abstract

PURPOSE: Computer-aided design/computer-integrated machining (CAD/CIM) allows defect-oriented custom-shaping of the inside surfaces of all-ceramic crowns. The purpose of this study was to examine the effect of inside crown form on fracture strength of cemented and bonded crowns.
MATERIALS AND METHODS: Four preparation types were used: (1) "classic" with a butt shoulder of 1.2 mm, abutment height of 4 mm, and 6-degree convergence, (2) like type 1 with mesio-occlusodistal cavity, (3) like type 1 with height reduced by 50%, and (4) like type 1 with abutment reduced by 100% plus a pulp chamber cavity. Crowns were CAD designed on preparations 1 to 4 using identical outside morphology. Machined crowns were placed on abutments (a) without any media as controls (n = 15), (b) cemented (n = 15), and (c) bonded (n = 15), and were loaded until fracture.
RESULTS: Zinc phosphate-cemented crowns (1b, 2b, 3b, and 4b) showed significant (P < 0.001) increase of fracture load values compared to uncemented control crowns (1a, 2a, 3a, 4a). Fracture load values of bonded crowns (1c, 2c, 3c) were significantly (P < 0.001) higher than those for cemented crowns. Bonded crowns with thick occlusal dimensions (3c and 4c) showed the highest fracture load values.
CONCLUSION: Bonded all-ceramic CAD/CIM crowns with defect-oriented inside morphology and increased occlusal dimensions showed high fracture load values.

Entities:  

Mesh:

Substances:

Year:  1998        PMID: 9758997

Source DB:  PubMed          Journal:  Int J Prosthodont        ISSN: 0893-2174            Impact factor:   1.681


  7 in total

Review 1.  All-ceramic crowns: bonding or cementing?

Authors:  Peter Pospiech
Journal:  Clin Oral Investig       Date:  2002-11-21       Impact factor: 3.573

2.  Computer-aided evaluation of preparations for CAD/CAM-fabricated all-ceramic crowns.

Authors:  Jan-Frederik Güth; Jan Wallbach; Michael Stimmelmayr; Wolfgang Gernet; Florian Beuer; Daniel Edelhoff
Journal:  Clin Oral Investig       Date:  2012-08-07       Impact factor: 3.573

3.  Fracture load of CAD/CAM-fabricated and 3D-printed composite crowns as a function of material thickness.

Authors:  Moritz Zimmermann; Andreas Ender; Gustav Egli; Mutlu Özcan; Albert Mehl
Journal:  Clin Oral Investig       Date:  2018-10-27       Impact factor: 3.573

4.  Internal fit of two all-ceramic systems and metal-ceramic crowns.

Authors:  Leandro Moura Martins; Fabio Cesar Lorenzoni; Alcides Oliveira de Melo; Luciana Mendonça de Silva; José Luiz G de Oliveira; Pedro Cesar Garcia de Oliveira; Gerson Bonfante
Journal:  J Appl Oral Sci       Date:  2012 Mar-Apr       Impact factor: 2.698

Review 5.  Endocrowns: review.

Authors:  Gaye Sevimli; Seda Cengiz; M Selcuk Oruc
Journal:  J Istanb Univ Fac Dent       Date:  2015-04-29

6.  Finite element analysis of adhesive endo-crowns of molars at different height levels of buccally applied load.

Authors:  Istabrak Hasan; Matthias Frentzen; Karl-Heinz Utz; Daniel Hoyer; Alexander Langenbach; Christoph Bourauel
Journal:  J Dent Biomech       Date:  2012-08-03

7.  Effect of cements on fracture resistance of monolithic zirconia crowns.

Authors:  Keisuke Nakamura; Mathieu Mouhat; John Magnus Nergård; Solveig Jenssen Lægreid; Taro Kanno; Percy Milleding; Ulf Örtengren
Journal:  Acta Biomater Odontol Scand       Date:  2016-01-26
  7 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.