Flexural strength of feldspathic porcelain treated with ion exchange, overglaze, and polishing.

R A Giordano1, S Campbell, R Pober.   

Abstract

Feldspathic porcelains, which are used in the construction of porcelain-fused-to-metal (PFM) restorations, have an inherent weakness because of their brittle nature and processing flaws. A relatively new product, the Tuf-Coat ion exchange system, claims to substantially strengthen feldspathic porcelains. This study compared the strengthening effect of the Tuf-Coat system with that of surface treatments such as overglazing, polishing, and finishing. Bend bars of Vita VMK 68 porcelain were made and randomly assigned to eight different surface treatment groups to examine these effects. The flexural strengths revealed that although Tuf-Coat treatment strengthened the porcelain, it was not significantly different from overglazing, and the strengthening effect was lost if the porcelain was subsequently self-glazed or finished.

Entities:  

Mesh:

Substances:

Year:  1994        PMID: 8006841     DOI: 10.1016/0022-3913(94)90184-8

Source DB:  PubMed          Journal:  J Prosthet Dent        ISSN: 0022-3913            Impact factor:   3.426


  6 in total

1.  An in vitro study to identify a ceramic polishing protocol effecting smoothness superior to glazed surface.

Authors:  Noxy George Manjuran; T Sreelal
Journal:  J Indian Prosthodont Soc       Date:  2013-08-22

2.  An in vitro investigation to compare the surface roughness of auto glazed, reglazed and chair side polished surfaces of Ivoclar and Vita feldspathic porcelain.

Authors:  Sumit Sethi; Dilip Kakade; Shantanu Jambhekar; Vinay Jain
Journal:  J Indian Prosthodont Soc       Date:  2012-12-14

3.  Effect of thermocycling on the flexural strength of porcelain laminate veneers.

Authors:  Deepa Subramanian; G Sivagami; D Sendhilnathan; Cs Rajmohan
Journal:  J Conserv Dent       Date:  2008-10

4.  Evaluation of efficiency of manual polishing over autoglazed and overglazed porcelain and its effect on plaque accumulation.

Authors:  Satheesh B Haralur
Journal:  J Adv Prosthodont       Date:  2012-11-29       Impact factor: 1.904

5.  An In vitro Evaluation to Compare the Surface Roughness of Glazed, Reglazed and Chair Side Polished Surfaces of Dental Porcelain.

Authors:  Varsha Rani; Sanjeev Mittal; Urvashi Sukhija
Journal:  Contemp Clin Dent       Date:  2021-06-14

6.  Shear bond strength of orthodontic buccal tubes to porcelain.

Authors:  Kathiravan Purmal; Mohammad K Alam; Prema Sukumaran
Journal:  Dent Res J (Isfahan)       Date:  2013-01
  6 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.