Late degradation tissue response to poly(L-lactide) bone plates and screws.

J E Bergsma1, W C de Bruijn, F R Rozema, R R Bos, G Boering.   

Abstract

Patients with fractures of the zygomatic bone were treated with high molecular weight poly(L-lactic) acid (PLLA) bone plates and screws. Three years after implantation four patients returned to our department with a swelling at the site of implantation. At the recall of the remaining patients we found an identical type of swelling after the same implantation period. To investigate the nature of the tissue reaction, eight patients were reoperated for the removal of the swelling. The implantation period of the PLLA material varied from 3.3 to 5.7 years. Microscopic evaluation and molecular weight measurements were performed. The excised material showed remnants of degraded PLLA material surrounded by a dense fibrous capsule. Ultrastructural investigation showed crystal-like PLLA material internalized by various cells. The results of this investigation suggest that the PLLA material slowly degrades into particles with a high crystallinity. The intra- and extracellular degradation rate of these particles is very low. After 5.7 years of implantation, these particles were still not fully resorbed.

Entities:  

Mesh:

Substances:

Year:  1995        PMID: 7718688     DOI: 10.1016/0142-9612(95)91092-d

Source DB:  PubMed          Journal:  Biomaterials        ISSN: 0142-9612            Impact factor:   12.479


  97 in total

1.  Complications of bioresorbable fixation systems in pediatric neurosurgery.

Authors:  Cherukuri Ravi Kumar; Sandeep Sood; Steven Ham
Journal:  Childs Nerv Syst       Date:  2004-07-29       Impact factor: 1.475

2.  Porous calcium sulfate ceramics with tunable degradation rate.

Authors:  Shu-Ting Kuo; Hao-Wei Wu; Wei-Hsing Tuan; Yu-Yu Tsai; Sea-Fue Wang; Yoshio Sakka
Journal:  J Mater Sci Mater Med       Date:  2012-07-03       Impact factor: 3.896

3.  Preparation and in vitro/in vivo evaluations of dimpled poly(L-lactic acid) fibers mixed/coated with hydroxyapatite nanocrystals.

Authors:  Hiroshi Yanagida; Masahiro Okada; Miwa Masuda; Isao Narama; Shigeyuki Nakano; Satoshi Kitao; Kazuo Takakuda; Tsutomu Furuzono
Journal:  J Artif Organs       Date:  2011-07-22       Impact factor: 1.731

4.  Recurrent locking of knee joint caused by intraarticular migration of bioabsorbable tibial interference screw after arthroscopic ACL reconstruction.

Authors:  Andreas Appelt; Martin Baier
Journal:  Knee Surg Sports Traumatol Arthrosc       Date:  2006-10-28       Impact factor: 4.342

5.  Will the hold of solid biodegradable implants be influenced by swelling during the degradation process? An in-vitro study with Meniscus Arrows.

Authors:  Diederick B Wouters; Rudolf R M Bos; Jeff T De Hosson
Journal:  Knee Surg Sports Traumatol Arthrosc       Date:  2007-06-23       Impact factor: 4.342

6.  Synthesis, characterization and cytocompatibility of a degradable polymer using ferric catalyst for esophageal tissue engineering.

Authors:  Yu-Na Lei; Ya-Bin Zhu; Chang-Feng Gong; Jing-Jing Lv; Chen Kang; Lin-Xi Hou
Journal:  J Mater Sci Mater Med       Date:  2013-10-23       Impact factor: 3.896

7.  Short-term in vitro and in vivo biocompatibility of a biodegradable polyurethane foam based on 1,4-butanediisocyanate.

Authors:  B van Minnen; M B M van Leeuwen; B Stegenga; J Zuidema; C E Hissink; T G van Kooten; R R M Bos
Journal:  J Mater Sci Mater Med       Date:  2005-03       Impact factor: 3.896

Review 8.  Frontal sinus fractures: a conservative shift.

Authors:  William M Weathers; Erik M Wolfswinkel; Daniel A Hatef; Edward I Lee; Rodger H Brown; Larry H Hollier
Journal:  Craniomaxillofac Trauma Reconstr       Date:  2013-06-26

9.  [In vivo study of degradation of poly-(D,L-) lactide and poly-(L-lactide-co-glycolide) osteosynthesis material].

Authors:  W Heidemann; J H Fischer; J Koebke; C Bussmann; K L Gerlach
Journal:  Mund Kiefer Gesichtschir       Date:  2003-09-20

10.  Osteointegration of poly(L: -lactic acid)PLLA and poly(L: -lactic acid)PLLA/poly(ethylene oxide)PEO implants in rat tibiae.

Authors:  Débora Cristina Coraça; Eliana Aparaecida R Duek; Carlos A Padovani; José Angelo Camilli
Journal:  J Mater Sci Mater Med       Date:  2008-02-19       Impact factor: 3.896

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.