Metallic wear in failed titanium-alloy total hip replacements. A histological and quantitative analysis.

H J Agins1, N W Alcock, M Bansal, E A Salvati, P D Wilson, P M Pellicci, P G Bullough.   

Abstract

We conducted extensive histological examination of the tissues that were adjacent to the prosthesis in nine hips that had a failed total arthroplasty. The prostheses were composed of titanium alloy (Ti-6Al-4V) and ultra-high molecular weight polyethylene. The average time that the prosthesis had been in place in the tissue was 33.5 months (range, eleven to fifty-seven months). Seven arthroplasties were revised because of aseptic loosening and two, for infection. In eight hips cement had been used and in one (that had a porous-coated implant for fifty-two months) no cement had been utilized. Intense histiocytic and plasma-cell reaction was noted in the pseudocapsular tissue. There was copious metallic staining of the lining cells. Polyethylene debris and particles of cement with concomitant giant-cell reaction were present in five hips. Atomic absorption spectrophotometry revealed values for titanium of fifty-sic to 3700 micrograms per gram of dry tissue (average, 1047 micrograms per gram; normal, zero microgram per gram), for aluminum of 2.1 to 396 micrograms per gram (average, 115 micrograms per gram; normal, zero micrograms per gram), and for vanadium of 2.9 to 220 micrograms per gram (average, sixty-seven micrograms per gram; normal, 1.2 micrograms per gram). The highest values were found in the hip in which surgical revision was performed at fifty-seven months. The concentrations of the three elements in the soft tissues were similar to those in the metal of the prostheses. The factors to which failure was attributed were: vertical orientation of the acetabular component (five hips), poor cementing technique on the femoral side (three hips), infection (two hips), and separation of a sintered pad made of pure titanium (one hip). A femoral component that is made of titanium alloy can undergo severe wear of the surface and on the stem, where it is loose, with liberation of potentially toxic local concentrations of metal debris into the surrounding tissues. It may contribute to infection and loosening.

Entities:  

Mesh:

Substances:

Year:  1988        PMID: 3279037

Source DB:  PubMed          Journal:  J Bone Joint Surg Am        ISSN: 0021-9355            Impact factor:   5.284


  29 in total

1.  Quantifying subtle but persistent peri-spine inflammation in vivo to submicron cobalt-chromium alloy particles.

Authors:  Nadim James Hallab; Frank W Chan; Megan L Harper
Journal:  Eur Spine J       Date:  2012-03-10       Impact factor: 3.134

2.  Quantitative analysis of the wear and wear debris from low and high carbon content cobalt chrome alloys used in metal on metal total hip replacements.

Authors:  J L Tipper; P J Firkins; E Ingham; J Fisher; M H Stone; R Farrar
Journal:  J Mater Sci Mater Med       Date:  1999-06       Impact factor: 3.896

3.  Implications of orthopedic fretting corrosion particles on skeletal muscle microcirculation.

Authors:  C N Kraft; B Burian; O Diedrich; M A Wimmer
Journal:  J Mater Sci Mater Med       Date:  2001 Oct-Dec       Impact factor: 3.896

4.  Modulation of the phenotypic and functional properties of phagocytic macrophages by wear particles from orthopaedic implants.

Authors:  N Al-Saffar; P A Revell; A Kobayashi
Journal:  J Mater Sci Mater Med       Date:  1997-11       Impact factor: 3.896

5.  Assessment of epidural versus intradiscal biocompatibility of PEEK implant debris: an in vivo rabbit model.

Authors:  Nadim J Hallab; Qi-Bin Bao; Tim Brown
Journal:  Eur Spine J       Date:  2013-08-31       Impact factor: 3.134

6.  Susceptibility of a polycaprolactone-based root canal filling material to degradation using an agar-well diffusion assay.

Authors:  Noriko Hiraishi; Fernanda T Sadek; Nigel M King; Marco Ferrari; David H Pashley; Franklin R Tay
Journal:  Am J Dent       Date:  2008-04       Impact factor: 1.522

7.  High failure rate of a modern, proximally roughened, cemented stem for total hip arthroplasty.

Authors:  A Grose; A González Della Valle; P Bullough; S Lyman; I Tomek; P Pellicci
Journal:  Int Orthop       Date:  2006-04-29       Impact factor: 3.075

Review 8.  Are clinical findings of systemic titanium dispersion following implantation explained by available in vitro evidence? An evidence-based analysis.

Authors:  Justin Paul Curtin; Minji Wang
Journal:  J Biol Inorg Chem       Date:  2017-05-17       Impact factor: 3.358

9.  Basic science considerations in primary total hip replacement arthroplasty.

Authors:  Saqeb B Mirza; Douglas G Dunlop; Sukhmeet S Panesar; Syed G Naqvi; Shafat Gangoo; Saif Salih
Journal:  Open Orthop J       Date:  2010-05-11

10.  Preliminary experience with biodegradable implants for fracture fixation.

Authors:  Mandeep S Dhillon; Sharad Prabhakar; Chandiralingam Prasanna
Journal:  Indian J Orthop       Date:  2008-07       Impact factor: 1.251

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.