| Literature DB >> 31927973 |
Il-Kwon Oh1,2, Li Zeng1, Jae-Eun Kim3,4, Jong-Seo Park2,5, Kangsik Kim6, Hyunsoo Lee3,4, Seunggi Seo2, Mohammad Rizwan Khan5, Sangmo Kim7, Chung Wung Park7, Junghoon Lee8, Bonggeun Shong9, Zonghoon Lee6, Stacey F Bent1, Hyungjun Kim2, Jeong Young Park3,4, Han-Bo-Ram Lee5.
Abstract
Fine-tuning of the surface free energy (SFE) of a solid material facilitates its use in a wide range of applications requiring precise control of the ubiquitous presence of liquid on the surface. In this study, we found that the SFE of rare-earth oxide (REO) thin films deposited by atomic layer deposition (ALD) gradually decreased with increasing film thickness; however, these changes could not be understood by classical interaction models. Herein, the mechanism underlying the aforesaid decrease was systematically studied by measuring contact angles, surface potential, adhesion force, crystalline structures, chemical compositions, and morphologies of the REO films. A growth mode of the REO films was observed: layer-by-layer growth at the initial stage with an amorphous phase and subsequent crystalline island growth, accompanied by a change in the crystalline structure and orientation that affects the SFE. The portion of the surface crystalline facets terminated with (222) and (440) planes evolved with an increase in ALD cycles and film thickness, as an amorphous phase was transformed. Based on this information, we demonstrated an SFE-tuned liquid tweezer with selectivity to target liquid droplets. We believe that the results of this fundamental and practical study, with excellent selectivity to liquids, will have significant impacts on coating technology.Entities:
Keywords: atomic layer deposition; metal oxides; phase transformation; rare-earth oxides; surface energy control
Year: 2020 PMID: 31927973 DOI: 10.1021/acsnano.9b07430
Source DB: PubMed Journal: ACS Nano ISSN: 1936-0851 Impact factor: 15.881