Evaluation of mechanical and optical behavior of current esthetic dental restorative CAD/CAM composites.

Bogna Stawarczyk1, Anja Liebermann2, Marlis Eichberger2, Jan-Frederik Güth2.   

Abstract

OBJECTIVES: To determine the mechanical and optical properties of CAD/CAM composites (LAVA Ultimate, Cerasmart, Shofu Block and two exp. CAD/CAM composites), a hybrid material (VITA Enamic), a leucite (IPS Empress CAD) and a lithium disilicate glass-ceramic (IPS e.max CAD).
MATERIALS AND METHODS: Three-point flexural strength (FS) was investigated according ISO 6872:2008 (N=240/n=30). Two-body wear (TBW) was analyzed in a chewing simulator (1,200,000 cycles, 50N, 5°/55°C) using human teeth as antagonists (N=120/n=15). Quantitative analysis of wear was carried out with a 3D-scanner and associated matching software. Discoloration rate (DR) after 14 days of storage in cress, curry, red wine, and distilled water (N=384/n=12), and translucency (T) (N=384/n=48) of CAD/CAM materials were measured in a spectrophotometer (400-700nm wavelength). Data were analyzed using two-/one-way ANOVA with Scheffé post-hoc test, Kruskal-Wallis-H test, and linear mixed models (α=0.05).
RESULTS: IPS e.max CAD showed the highest FS (p<0.001), followed by LAVA Ultimate; however, not different from the remaining CAD/CAM composites (exception: Shofu Block). The lowest FS showed VITA Enamic and IPS Empress CAD (p<0.001). IPS Empress CAD, VITA Enamic, exp. CAD/CAM composite 2, followed by IPS e.max presented lower material TBW than the remaining CAD/CAM materials (p<0.001). The highest antagonist wear was observed for the tested glass-ceramics and the hybrid material (p<0.001). Storage medium (red wine>curry>cress>distilled water) exerted the highest influence on DR (p<0.001), closely followed by CAD/CAM material. Glass-ceramics showed lower DR than CAD/CAM composites (p<0.001).
CONCLUSIONS: CAD/CAM composites presented moderate FS, high T and antagonist friendly behavior. Glass-ceramic demonstrated the most favorable DR and lowest TBW on the material side.
Copyright © 2015 Elsevier Ltd. All rights reserved.

Entities:  

Keywords:  CAD/CAM composite; Discoloration; Optical and mechanical properties; Three-point flexural strength; Two-body wear

Mesh:

Substances:

Year:  2015        PMID: 26519658     DOI: 10.1016/j.jmbbm.2015.10.004

Source DB:  PubMed          Journal:  J Mech Behav Biomed Mater        ISSN: 1878-0180


  29 in total

1.  The flexural strength of CAD/CAM polymer crowns and the effect of artificial ageing on the fracture resistance of CAD/CAM polymer and ceramic single crowns.

Authors:  Anna Winter; Axel Schurig; Engelke Rasche; Franziska Rösner; Lisa Kanus; Marc Schmitter
Journal:  J Mater Sci Mater Med       Date:  2019-12-23       Impact factor: 3.896

2.  Sliding contact wear and subsurface damage of CAD/CAM materials against zirconia.

Authors:  M Wendler; M R Kaizer; R Belli; U Lohbauer; Y Zhang
Journal:  Dent Mater       Date:  2020-01-30       Impact factor: 5.304

3.  Polymer infiltrated ceramic network structures for resistance to fatigue fracture and wear.

Authors:  Haifa El Zhawi; Marina R Kaizer; Asima Chughtai; Rafael R Moraes; Yu Zhang
Journal:  Dent Mater       Date:  2016-08-29       Impact factor: 5.304

4.  Chair-side generated posterior monolithic lithium disilicate crowns: clinical survival after 6 years.

Authors:  Angelika Rauch; Sven Reich; Oliver Schierz
Journal:  Clin Oral Investig       Date:  2016-11-28       Impact factor: 3.573

5.  Polymer-infiltrated ceramic CAD/CAM inlays and partial coverage restorations: 3-year results of a prospective clinical study over 5 years.

Authors:  F A Spitznagel; K J Scholz; J R Strub; K Vach; P C Gierthmuehlen
Journal:  Clin Oral Investig       Date:  2017-12-06       Impact factor: 3.573

6.  Effect of Miswak Derivatives on Color Changes and Mechanical Properties of Polymer-Based Computer-Aided Design and Computer-Aided Manufactured (CAD/CAM) Dental Ceramic Materials.

Authors:  Manea M Al-Ahmari; Abdulrahman H Alzahrani; Feras A Al-Qatarneh; Mohammed M Al Moaleem; Mansoor Shariff; Saeed M Alqahtani; Amit Porwal; Fuad A Al-Sanabani; Thiyezen A AlDhelai
Journal:  Med Sci Monit       Date:  2022-06-17

Review 7.  "Digitally Oriented Materials": Focus on Lithium Disilicate Ceramics.

Authors:  Fernando Zarone; Marco Ferrari; Francesco Guido Mangano; Renato Leone; Roberto Sorrentino
Journal:  Int J Dent       Date:  2016-08-18

8.  The effects of different polishing techniques on the staining resistance of CAD/CAM resin-ceramics.

Authors:  Omer Sagsoz; Tevfik Demirci; Gamze Demirci; Nurdan Polat Sagsoz; Mehmet Yildiz
Journal:  J Adv Prosthodont       Date:  2016-12-15       Impact factor: 1.904

9.  In Vitro Investigation of Wear of CAD/CAM Polymeric Materials Against Primary Teeth.

Authors:  Jae-Won Choi; Eun-Ju Song; Jong-Hyun Shin; Tae-Sung Jeong; Jung-Bo Huh
Journal:  Materials (Basel)       Date:  2017-12-09       Impact factor: 3.623

10.  In-vivo-wear in composite and ceramic full mouth rehabilitations over 3 years.

Authors:  Gintare Burian; Kurt Erdelt; Josef Schweiger; Christine Keul; Daniel Edelhoff; Jan-Frederik Güth
Journal:  Sci Rep       Date:  2021-07-07       Impact factor: 4.379

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.