Evaluation of the bond strength of resin cements used to lute ceramics on laser-etched dentin.

Figen Eren Giray1, Lale Duzdar, Mustafa Oksuz, Ilknur Tanboga.   

Abstract

OBJECTIVE: The purpose of this study was to investigate the shear bond strength (SBS) of two different adhesive resin cements used to lute ceramics on laser-etched dentin. BACKGROUND DATA: Erbium, chromium: yttrium, scandium, gallium, garnet (Er,Cr:YSGG) laser irradiation has been claimed to improve the adhesive properties of dentin, but results to date have been controversial, and its compatibility with existing adhesive resin cements has not been conclusively determined.
MATERIALS AND METHODS: Two adhesive cements, one "etch-and-rinse" [Variolink II (V)] and one "self-etch" [Clearfil Esthetic Cement (C)] luting cement, were used to lute ceramic blocks (Vita Celay Blanks, Vita) onto dentin surfaces. In total, 80 dentin specimens were distributed randomly into eight experimental groups according to the dentin surface-etching technique used Er,Cr:YSGG laser and Er:YAG laser: (1) 37% orthophosphoric acid+V (control group), (2) Er,Cr:YSGG laser+V, (3) Er,Cr:YSGG laser+acid+V, (4) Er:YAG laser+V, (5) Er:YAG laser+acid+V, (6) C, (7) Er,Cr:YSGG laser+C, and (8) Er:YAG laser+C. Following these applications, the ceramic discs were bonded to prepared surfaces and were shear loaded in a universal testing machine until fracture. SBS was recorded for each group in MPa. Shear test values were evaluated statistically using the Mann-Whitney U test.
RESULTS: No statistically significant differences were evident between the control group and the other groups (p>0.05). The Er,Cr:YSGG laser+A+V group demonstrated significantly higher SBS than did the Er,Cr:YSGG laser+V group (p=0.034). The Er,Cr:YSGG laser+C and Er:YAG laser+C groups demonstrated significantly lower SBS than did the C group (p<0.05).
CONCLUSIONS: Dentin surfaces prepared with lasers may provide comparable ceramic bond strengths, depending upon the adhesive cement used.

Entities:  

Mesh:

Substances:

Year:  2014        PMID: 24992276      PMCID: PMC4082358          DOI: 10.1089/pho.2013.3701

Source DB:  PubMed          Journal:  Photomed Laser Surg        ISSN: 1549-5418            Impact factor:   2.796


  34 in total

1.  Bonding to Er-YAG-laser-treated dentin.

Authors:  L Ceballo; M Toledano; R Osorio; F R Tay; G W Marshall
Journal:  J Dent Res       Date:  2002-02       Impact factor: 6.116

Review 2.  Posterior resin-based composite restorations: clinical recommendations for optimal success.

Authors:  A V Ritter
Journal:  J Esthet Restor Dent       Date:  2001       Impact factor: 2.843

3.  In vitro study of enamel and dentin marginal integrity of composite and compomer restorations placed in primary teeth after diamond or Er:YAG laser cavity preparation.

Authors:  M Stiesch-Scholz; M Hannig
Journal:  J Adhes Dent       Date:  2000       Impact factor: 2.359

4.  Compositional and structural changes of human dentin following caries removal by Er,Cr:YSGG laser irradiation in primary teeth.

Authors:  Mozammal Hossain; Yukio Nakamura; Yoshishige Yamada; Yoshiko Murakami; Koukichi Matsumoto
Journal:  J Clin Pediatr Dent       Date:  2002       Impact factor: 1.065

5.  Shear bond strength of composite bonded to erbium:yttrium-aluminum-garnet laser-prepared dentin.

Authors:  Sevil Gurgan; Arlin Kiremitci; Filiz Yalcin Cakir; Esra Yazici; Jale Gorucu; Norbert Gutknecht
Journal:  Lasers Med Sci       Date:  2007-12-12       Impact factor: 3.161

6.  The impact of Er,Cr:YSGG laser on the shear strength of the bond between dentin and ceramic is dependent on the adhesive material.

Authors:  Barbara Cvikl; Gundula Moser; Jörg Wernisch; Modesto Raabe; Reinhard Gruber; Andreas Moritz
Journal:  Lasers Med Sci       Date:  2011-07-20       Impact factor: 3.161

7.  Effect of Er:YAG laser application on the shear bond strength and microleakage between resin cements and Y-TZP ceramics.

Authors:  Hakan Akin; Faik Tugut; Gulsah Emine Akin; Umit Guney; Burcu Mutaf
Journal:  Lasers Med Sci       Date:  2011-01-21       Impact factor: 3.161

8.  Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic.

Authors:  Raquel Castillo de Oyagüe; Francesca Monticelli; Manuel Toledano; Estrella Osorio; Marco Ferrari; Raquel Osorio
Journal:  Dent Mater       Date:  2008-07-14       Impact factor: 5.304

9.  Erbium, chromium:yttrium scandium gallium garnet laser for caries removal: influence on bonding of a self-etching adhesive system.

Authors:  Arlene Tachibana; Márcia Martins Marques; Julia Maria Pavan Soler; Adriana Bona Matos
Journal:  Lasers Med Sci       Date:  2007-10-26       Impact factor: 3.161

10.  Bond strength durability of self-etching adhesives and resin cements to dentin.

Authors:  Carolina de Andrade Lima Chaves; Renata Marques de Melo; Sheila Pestana Passos; Fernanda Pelógia Camargo; Marco Antonio Bottino; Ivan Balducci
Journal:  J Appl Oral Sci       Date:  2009 May-Jun       Impact factor: 2.698

View more
  6 in total

1.  Evaluation of bond strength of resin cement to Er:YAG laser-etched enamel and dentin after cementation of ceramic discs.

Authors:  Artur Ismatullaev; Simge Taşın; Aslihan Usumez
Journal:  Lasers Med Sci       Date:  2020-07-22       Impact factor: 3.161

2.  The use of Erbium: Yttrium-aluminum-garnet laser in cavity preparation and surface treatment: 3-year follow-up.

Authors:  Isil Buyukhatipoglu; Asli Secilmis
Journal:  Eur J Dent       Date:  2015 Apr-Jun

3.  Effect of Er,Cr:YSGG Laser at Different Output Powers on the Micromorphology and the Bond Property of Non-Carious Sclerotic Dentin to Resin Composites.

Authors:  Xiang Sun; Jinghao Ban; Xinjia Sha; Weiguo Wang; Yang Jiao; Wanshan Wang; Yanwei Yang; Jingjing Wei; Lijuan Shen; Jihua Chen
Journal:  PLoS One       Date:  2015-11-06       Impact factor: 3.240

Review 4.  Cementation of Glass-Ceramic Posterior Restorations: A Systematic Review.

Authors:  Carline R G van den Breemer; Marco M M Gresnigt; Marco S Cune
Journal:  Biomed Res Int       Date:  2015-10-18       Impact factor: 3.411

5.  Effect of Surface Treatments on the Shear Bond Strength of Indirect Esthetic Restorative Materials to Dentin.

Authors:  Dhuha M Masri; Nisreen S Alghamdi; Najoud S Alhawiti; Renad M Alawi; Shroug K Alhothari; Salah A Yousief; Mahmoud A Mekky
Journal:  Open Access Maced J Med Sci       Date:  2019-08-11

6.  Dentin bond strength of bioactive cement in comparison to conventional resin cement when photosensitized with Er,Cr:YSGG Laser.

Authors:  Fahad Alkhudhairy; Sulieman S Al-Johany; Mustafa Naseem; Mohammed Bin-Shuwaish; Fahim Vohra
Journal:  Pak J Med Sci       Date:  2020 Jan-Feb       Impact factor: 1.088

  6 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.