Literature DB >> 22592165

Effect of quaternary ammonium and silver nanoparticle-containing adhesives on dentin bond strength and dental plaque microcosm biofilms.

Ke Zhang1, Mary Anne S Melo, Lei Cheng, Michael D Weir, Yuxing Bai, Hockin H K Xu.   

Abstract

OBJECTIVE: Antibacterial bonding agents are promising to hinder the residual and invading bacteria at the tooth-restoration interfaces. The objectives of this study were to develop an antibacterial bonding agent by incorporation of n>an class="Chemical">quaternary ammonium dimethacrylate (QADM) and nanoparticles of silver (NAg), and to investigate the effect of QADM-NAg adhesive and primer on dentin bond strength and plaque microcosm biofilm response for the first time.
METHODS: Scotchbond Multi-Purpose adhesive and primer were used as control. Experimental adhesive and primer were made by adding QADM and NAg into control adhesive and primer. Human dentin shear bond strengths were measured (n = 10). A dental plaque microcosm biofilm model with human saliva as inoculum was used to investigate biofilm metabolic activity, colony-forming unit (CFU) counts, lactic acid production, and live/dead staining assay (n = 6).
RESULTS: Adding QADM and NAg into adhesive and primer did not compromise the dentin shear bond strength which ranged from 30 to 35MPa (p>0.1). Scanning electron microscopy (SEM) examinations revealed numerous resin tags, which were similar for the control and the QADM and NAg groups. Adding QADM or NAg markedly reduced the biofilm viability, compared to adhesive control. QADM and NAg together in the adhesive had a much stronger antibacterial effect than using each agent alone (p<0.05). Adding QADM and NAg in both adhesive and primer had the strongest antibacterial activity, reducing metabolic activity, CFU, and lactic acid by an order of magnitude, compared to control. SIGNIFICANCE: Without compromising dentin bond strength and resin tag formation, the QADM and NAg containing adhesive and primer achieved strong antibacterial effects against microcosm biofilms for the first time. QADM-NAg adhesive and primer are promising to combat residual bacteria in tooth cavity and invading bacteria at the margins, thereby to inhibit secondary caries. QADM and NAg incorporation may have a wide applicability to other dental bonding systems.
Copyright © 2012 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2012        PMID: 22592165      PMCID: PMC3393841          DOI: 10.1016/j.dental.2012.04.027

Source DB:  PubMed          Journal:  Dent Mater        ISSN: 0109-5641            Impact factor:   5.304


  56 in total

Review 1.  Antibacterial properties of resin composites and dentin bonding systems.

Authors:  Satoshi Imazato
Journal:  Dent Mater       Date:  2003-09       Impact factor: 5.304

2.  Antibacterial activity of dentine primer containing MDPB after curing.

Authors:  S Imazato; A Ehara; M Torii; S Ebisu
Journal:  J Dent       Date:  1998-03       Impact factor: 4.379

3.  Antibacterial activity of dental composites containing quaternary ammonium polyethylenimine nanoparticles against Streptococcus mutans.

Authors:  Nurit Beyth; Ira Yudovin-Farber; Ran Bahir; Abraham J Domb; Ervin I Weiss
Journal:  Biomaterials       Date:  2006-03-27       Impact factor: 12.479

4.  Development of an antimicrobial resin--a pilot study.

Authors:  Catherine Fan; Lianrui Chu; H Ralph Rawls; Barry K Norling; Hector L Cardenas; Kyumin Whang
Journal:  Dent Mater       Date:  2010-11-26       Impact factor: 5.304

5.  Hygroscopic dimensional changes of self-adhering and new resin-matrix composites during water sorption/desorption cycles.

Authors:  Yong-jie Wei; Nick Silikas; Zhen-ting Zhang; David C Watts
Journal:  Dent Mater       Date:  2010-11-26       Impact factor: 5.304

6.  In vitro antibacterial effects of the dentin primer of Clearfil Protect Bond.

Authors:  Satoshi Imazato; Akiko Kuramoto; Yusuke Takahashi; Shigeyuki Ebisu; Mathilde C Peters
Journal:  Dent Mater       Date:  2005-09-29       Impact factor: 5.304

7.  In situ formation of silver nanoparticles in photocrosslinking polymers.

Authors:  Ya-Jun Cheng; Diana N Zeiger; John A Howarter; Xinran Zhang; Nancy J Lin; Joseph M Antonucci; Sheng Lin-Gibson
Journal:  J Biomed Mater Res B Appl Biomater       Date:  2011-02-02       Impact factor: 3.368

8.  AMORPHOUS CALCIUM PHOSPHATE COMPOSITES AND THEIR EFFECT ON COMPOSITE-ADHESIVE-DENTIN BONDING.

Authors:  J M Antonucci; J N R O'Donnell; G E Schumacher; D Skrtic
Journal:  J Adhes Sci Technol       Date:  2009-01-01       Impact factor: 2.077

Review 9.  Degradation, fatigue, and failure of resin dental composite materials.

Authors:  J L Drummond
Journal:  J Dent Res       Date:  2008-08       Impact factor: 6.116

10.  In vitro analysis of inhibitory effects of the antibacterial monomer MDPB-containing restorations on the progression of secondary root caries.

Authors:  Thaís Thomé; Marcia P A Mayer; Satoshi Imazato; Vinícius R Geraldo-Martins; Márcia M Marques
Journal:  J Dent       Date:  2009-05-28       Impact factor: 4.379

View more
  60 in total

Review 1.  Nanotechnology strategies for antibacterial and remineralizing composites and adhesives to tackle dental caries.

Authors:  Lei Cheng; Ke Zhang; Michael D Weir; Mary Anne S Melo; Xuedong Zhou; Hockin H K Xu
Journal:  Nanomedicine (Lond)       Date:  2015-03       Impact factor: 5.307

2.  Dual antibacterial agents of nano-silver and 12-methacryloyloxydodecylpyridinium bromide in dental adhesive to inhibit caries.

Authors:  Ke Zhang; Fang Li; Satoshi Imazato; Lei Cheng; Huaibing Liu; Dwayne D Arola; Yuxing Bai; Hockin H K Xu
Journal:  J Biomed Mater Res B Appl Biomater       Date:  2013-03-26       Impact factor: 3.368

3.  Effects of dual antibacterial agents MDPB and nano-silver in primer on microcosm biofilm, cytotoxicity and dentine bond properties.

Authors:  Ke Zhang; Lei Cheng; Satoshi Imazato; Joseph M Antonucci; Nancy J Lin; Sheng Lin-Gibson; Yuxing Bai; Hockin H K Xu
Journal:  J Dent       Date:  2013-02-08       Impact factor: 4.379

4.  Effect of water-ageing on dentine bond strength and anti-biofilm activity of bonding agent containing new monomer dimethylaminododecyl methacrylate.

Authors:  Ke Zhang; Lei Cheng; Eric J Wu; Michael D Weir; Yuxing Bai; Hockin H K Xu
Journal:  J Dent       Date:  2013-04-10       Impact factor: 4.379

5.  Hydrophilicity of dentin bonding systems influences in vitro Streptococcus mutans biofilm formation.

Authors:  Eugenio Brambilla; Andrei Ionescu; Annalisa Mazzoni; Milena Cadenaro; Massimo Gagliani; Monica Ferraroni; Franklin Tay; David Pashley; Lorenzo Breschi
Journal:  Dent Mater       Date:  2014-06-19       Impact factor: 5.304

6.  Effect of salivary pellicle on antibacterial activity of novel antibacterial dental adhesives using a dental plaque microcosm biofilm model.

Authors:  Fang Li; Michael D Weir; Ashraf F Fouad; Hockin H K Xu
Journal:  Dent Mater       Date:  2013-12-11       Impact factor: 5.304

7.  Three-dimensional biofilm properties on dental bonding agent with varying quaternary ammonium charge densities.

Authors:  Han Zhou; Huaibing Liu; Michael D Weir; Mark A Reynolds; Ke Zhang; Hockin H K Xu
Journal:  J Dent       Date:  2016-07-26       Impact factor: 4.379

8.  Effects of antibacterial primers with quaternary ammonium and nano-silver on Streptococcus mutans impregnated in human dentin blocks.

Authors:  Lei Cheng; Ke Zhang; Michael D Weir; Huaibing Liu; Xuedong Zhou; Hockin H K Xu
Journal:  Dent Mater       Date:  2013-02-17       Impact factor: 5.304

9.  Comparison of quaternary ammonium-containing with nano-silver-containing adhesive in antibacterial properties and cytotoxicity.

Authors:  Fang Li; Michael D Weir; Jihua Chen; Hockin H K Xu
Journal:  Dent Mater       Date:  2013-02-18       Impact factor: 5.304

10.  Dental primer and adhesive containing a new antibacterial quaternary ammonium monomer dimethylaminododecyl methacrylate.

Authors:  Lei Cheng; Michael D Weir; Ke Zhang; Dwayne D Arola; Xuedong Zhou; Hockin H K Xu
Journal:  J Dent       Date:  2013-01-23       Impact factor: 4.379

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.