An electron microscopic evaluation of the enamel surface subsequent to various debonding procedures.

S Howell1, W T Weekes.   

Abstract

In this study, enamel surface roughness was investigated following the use of various combinations of bonding agents, burrs and polishing procedures. Orthodontic brackets were bonded to 135 premolar teeth extracted from adolescents. Subsequent to debonding and finishing, the enamel surface was gold coated and examined in the scanning electron microscope. Each 200x photomicrograph was graded according to surface roughness and assigned to one of four selected standard grades. The use of different composites and different burs showed no significant effect on the finish of the enamel surface using Chi-square tests. Only two finishing procedures had a significant effect on surface roughness. The use of a Soflex disc followed by pumice slurry resulted in the roughest enamel surface and the use of pumice alone produced the smoothest enamel surface.

Mesh:

Substances:

Year:  1990        PMID: 2203330     DOI: 10.1111/j.1834-7819.1990.tb05402.x

Source DB:  PubMed          Journal:  Aust Dent J        ISSN: 0045-0421            Impact factor:   2.291


  13 in total

1.  Qualitative and quantitative evaluation of human dental enamel after bracket debonding: a noncontact three-dimensional optical profilometry analysis.

Authors:  Fabiano G Ferreira; Darcy F Nouer; Nelson P Silva; Ivana U Garbui; Lourenço Correr-Sobrinho; Paulo R A Nouer
Journal:  Clin Oral Investig       Date:  2013-12-11       Impact factor: 3.573

2.  Roughness of enamel surfaces after different bonding and debonding procedures : An in vitro study.

Authors:  Lorenz M Brauchli; Eva-Maria Baumgartner; Judith Ball; Andrea Wichelhaus
Journal:  J Orofac Orthop       Date:  2011-03-11       Impact factor: 1.938

3.  The influence of dental loupes on the quality of adhesive removal in orthodontic debonding.

Authors:  Denis F Baumann; Lorenz Brauchli; Hubertus van Waes
Journal:  J Orofac Orthop       Date:  2011-04-20       Impact factor: 1.938

4.  Enamel surface roughness after debonding.

Authors:  Sevinc Karan; Beyza Hancioglu Kircelli; Bahar Tasdelen
Journal:  Angle Orthod       Date:  2010-11       Impact factor: 2.079

5.  Evaluation of Enamel Roughness in Vitro After Orthodontic Bracket Debonding Using Different Methods of Residual Adhesive Removal.

Authors:  José Tarcísio Lima Ferreira; Maria Cristina Borsatto; Maria Conceição Pereira Saraiva; Mírian Aiko Nakane Matsumoto; Carolina Paes Torres; Fabio Lourenço Romano
Journal:  Turk J Orthod       Date:  2020-03-01

6.  Effects of removing adhesive from tooth surfaces by Er:YAG laser and a composite bur on enamel surface roughnessand pulp chamber temperature.

Authors:  Sogra Yassaei; Hossein Aghili; Neda Joshan
Journal:  Dent Res J (Isfahan)       Date:  2015 May-Jun

Review 7.  Effect of orthodontic debonding and adhesive removal on the enamel - current knowledge and future perspectives - a systematic review.

Authors:  Joanna Janiszewska-Olszowska; Tomasz Szatkiewicz; Robert Tomkowski; Katarzyna Tandecka; Katarzyna Grocholewicz
Journal:  Med Sci Monit       Date:  2014-10-20

8.  Effect of enamel laser irradiation at different pulse settings on shear bond strength of orthodontic brackets.

Authors:  Serkan Sağır; Aslıhan Usumez; Ebru Ademci; Serdar Usumez
Journal:  Angle Orthod       Date:  2013-06-13       Impact factor: 2.079

9.  The effects of composite resin types and debonding pliers on the amount of adhesive remnants and enamel damages: a stereomicroscopic evaluation.

Authors:  Parisa Salehi; Hamidreza Pakshir; Navid Naseri; Tahereh Baherimoghaddam
Journal:  J Dent Res Dent Clin Dent Prospects       Date:  2013-12-18

10.  Comparison of finishing and polishing systems for residual resin removal after debonding.

Authors:  Caöry Ulusoy
Journal:  J Appl Oral Sci       Date:  2009 May-Jun       Impact factor: 2.698

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.