A new method to test the fracture probability of all-ceramic crowns with a dual-axis chewing simulator.

S D Heintze1, T Albrecht, A Cavalleri, M Steiner.   

Abstract

OBJECTIVES: The purpose of this study was to validate a new laboratory method to test all-ceramic systems with regard to the proportion of failures.
METHODS: Sixteen standardized mandibular molar crowns consisting of two different materials (IPS Empress, IPS e.max Press) were adhesively luted on CAD/CAM milled PMMA abutments (first lower molar, circular chamfer). All crowns were loaded applying an eccentric force in a Willytec chewing simulator (steel stylus, Ø 2.4 mm, 2 mm lateral movement from fossa to cuspal tip) with stepwise increase of the load (3, 5, 9 kg, 100,000 cycles each, 0.8 Hz) and simultaneous thermocycling (5°C/55°C×417 per phase). Another four crowns of each material were subjected to force measurements with a 3D force sensor during dynamic loading of each loading phase using two different lateral movements (from fossa to cusp and vice versa).
RESULTS: The cumulative forces for the three directions in space were much higher compared to the static load of the chewing simulator (maximal force at 3 kg 60 N, 5 kg 160 N, 9 kg 240 N). There was no statistically significant difference in the mean or maximal force between the two materials or two different lateral movements. During dynamic loading, no fractures occurred in the molar crowns made of IPS e.max Press, whereas 50% of the IPS Empress crowns showed failures (75% fractures and 25% chippings) (log-rank test p=0.002). Most of the Empress crowns fractured during the third loading phase (9 kg).
CONCLUSIONS: The forces that the dead weights exerted during dynamic loading were 2-3 times higher than those during static loading. None of the lithium disilicate ceramic molar crowns fractured, whereas half of the leucite reinforced molar crowns failed during dynamic loading. Copyright Â
© 2010 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2010        PMID: 20932564     DOI: 10.1016/j.dental.2010.09.004

Source DB:  PubMed          Journal:  Dent Mater        ISSN: 0109-5641            Impact factor:   5.304


  9 in total

Review 1.  Ocular prosthesis incorporating IPS e-max press scleral veneer and a literature review on non-integrated ocular prosthesis.

Authors:  Godwin Clovis Da Costa; Meena Ajay Aras; Paul Chalakkal; Michelle Clovis Da Costa
Journal:  Int J Ophthalmol       Date:  2017-01-18       Impact factor: 1.779

2.  Reliability of reduced-thickness and thinly veneered lithium disilicate crowns.

Authors:  N R F A Silva; E A Bonfante; L M Martins; G B Valverde; V P Thompson; J L Ferencz; P G Coelho
Journal:  J Dent Res       Date:  2011-12-28       Impact factor: 6.116

Review 3.  Systematic review of chewing simulators: Reality and reproducibility of in vitro studies.

Authors:  Sergio Soriano-Valero; Juan-Luis Román-Rodriguez; Rubén Agustín-Panadero; Carlos Bellot-Arcís; Antonio Fons-Font; Lucía Fernández-Estevan
Journal:  J Clin Exp Dent       Date:  2020-12-01

4.  Fracture Resistance of Zirconia-Reinforced Lithium Silicate Ceramic Crowns Cemented with Conventional or Adhesive Systems: An In Vitro Study.

Authors:  Gianmaria D'Addazio; Manlio Santilli; Marco Lorenzo Rollo; Paolo Cardelli; Imena Rexhepi; Giovanna Murmura; Nadin Al-Haj Husain; Bruna Sinjari; Tonino Traini; Mutlu Özcan; Sergio Caputi
Journal:  Materials (Basel)       Date:  2020-04-25       Impact factor: 3.623

5.  Two-body wear of occlusal splint materials against different antagonists.

Authors:  Kubra Yildiz Domanic; Yilmaz Umut Aslan; Yasemin Ozkan
Journal:  BMC Oral Health       Date:  2020-06-22       Impact factor: 2.757

6.  Effects of dynamic aging on the wear and fracture strength of monolithic zirconia restorations.

Authors:  Işıl Sarıkaya; Yeliz Hayran
Journal:  BMC Oral Health       Date:  2018-08-23       Impact factor: 2.757

7.  The Structural Integrity and Fracture Behaviour of Teeth Restored with PEEK and Lithium-Disilicate Glass Ceramic Crowns.

Authors:  Sami Aldhuwayhi; Muhammad Syafiq Alauddin; Nicolas Martin
Journal:  Polymers (Basel)       Date:  2022-03-01       Impact factor: 4.329

8.  Simulation of clinical fractures for three different all-ceramic crowns.

Authors:  Marit Oilo; Ketil Kvam; Nils R Gjerdet
Journal:  Eur J Oral Sci       Date:  2014-04-04       Impact factor: 2.612

9.  Effect of lithium disilicate ceramic thickness, shade and translucency on transmitted irradiance and knoop microhardness of a light cured luting resin cement.

Authors:  Lincoln Pires Silva Borges; Gilberto Antônio Borges; Américo Bortolazzo Correr; Jeffrey A Platt; Sidney Kina; Lourenço Correr-Sobrinho; Ana Rosa Costa
Journal:  J Mater Sci Mater Med       Date:  2021-07-31       Impact factor: 3.896

  9 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.