The methods for the generation of smoothness in dental ceramics.

Kerem Yilmaz1, Pelin Ozkan.   

Abstract

Occlusal corrections, acidulated phosphate fluoride applications, carbonated beverages, or air-powder abrasion procedures can roughen the surface of restorations. Once deteriorated, porcelain surfaces need to be repolished. These surfaces can be reglazed or polished through various intraoral and extraoral polishing kits. Although clinicians often seek studies on the effect of repeated firings on coherence between metal and ceramic, the color of the porcelain, fluorescence, microstructure, and brightness, only a limited number of studies are available in the literature. This article reviews the available literature and presents methods for generating a smooth surface and assessing surface roughness. It also discusses the differences between glazing and mechanical polishing, highlighting the importance of mechanical polishing of dental ceramics.

Entities:  

Mesh:

Substances:

Year:  2010        PMID: 20158015

Source DB:  PubMed          Journal:  Compend Contin Educ Dent        ISSN: 1548-8578


  7 in total

1.  Comparative evaluation of the efficiency of four ceramic finishing systems.

Authors:  Prasad Aravind; P Abdul Razak; P G Francis; Johnson K Issac; R P Shanoj; T P Sasikumar
Journal:  J Int Oral Health       Date:  2013-10-26

2.  Surface treatment of dental porcelain: CO2 laser as an alternative to oven glaze.

Authors:  Ricardo Sgura; Mariana Cavalcante Reis; Antonio Carlos Hernandes; Márcia Carvalho de Abreu Fantini; Marcello Rubens Barsi Andreeta; Igor Studart Medeiros
Journal:  Lasers Med Sci       Date:  2013-07-24       Impact factor: 3.161

3.  Do thermal treatments affect the mechanical behavior of porcelain-veneered zirconia? A systematic review and meta-analysis.

Authors:  Camila da Silva Rodrigues; Iana Lamadrid Aurélio; Marina da Rosa Kaizer; Yu Zhang; Liliana Gressler May
Journal:  Dent Mater       Date:  2019-03-04       Impact factor: 5.304

4.  Effect finishing and polishing procedures on the surface roughness of IPS Empress 2 ceramic.

Authors:  Juliana Maria Capelozza Boaventura; Rodrigo Nishida; André Afif Elossais; Darlon Martins Lima; José Mauricio Santos Nunes Reis; Edson Alves Campos; Marcelo Ferrarezi de Andrade
Journal:  Acta Odontol Scand       Date:  2012-06-25       Impact factor: 2.331

5.  Effect of different coloring techniques and surface treatment methods on the surface roughness of monolithic zirconia.

Authors:  Rashin Giti; Shekoofeh Haghdoost; Elham Ansarifard
Journal:  Dent Res J (Isfahan)       Date:  2020-03-17

6.  The effect of repeated firings on the color change and surface roughness of dental ceramics.

Authors:  Fehmi Gonuldas; Kerem Yılmaz; Caner Ozturk
Journal:  J Adv Prosthodont       Date:  2014-08-14       Impact factor: 1.904

7.  Adhesion of Streptococcus Mutans to Glass Ionomer, BisCem Cement and Enamel: An in Vitro Study.

Authors:  Ezzatollah Jalalian; Ghazal Mofrad; Sogol Ahmadpour
Journal:  J Dent (Tehran)       Date:  2015-09
  7 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.