Bor-Shiunn Lee1, Shu-Han Kang, Yin-Lin Wang, Feng-Huei Lin, Chun-Pin Lin.
Abstract
DP-bioglass paste has been demonstrated to produce 60 microm of sealing depth on exposed dentinal tubules. However, the occlusive effect depended on a continuous placement of DP-bioglass paste on dentinal surface for three days. In a bid to fabricate highly reactive DP-bioglass particles, a sol-gel method was used together with HNO3, NaOH, and H3PO4 as catalysts. As a result, the application time of DP-bioglass paste was significantly reduced to 10 minutes. Percentage of tubular occlusion with DP-bioglass was 53.2-65.4%, while One Coat Bond and Seal & Protect yielded 51.3% and 41.2% respectively. Further, the average depth of tubular occlusion with DP-bioglass was 55.8-62.7 microm, while One Coat Bond and Seal & Protect produced 40.8 microm and 32.5 microm respectively. In conclusion, the best sealing performance of tubular occlusion was rendered by DP-bioglass catalyzed with HNO3. Its performance was significantly better than Seal & Protect, and was considered to exhibit the greatest potential in treating dentin hypersensitivity.Entities:
Mesh:
Substances:
Year: 2007 PMID: 17410893 DOI: 10.4012/dmj.26.52
Source DB: PubMed Journal: Dent Mater J ISSN: 0287-4547 Impact factor: 2.102