Determination of quantitative leucite content in pressable ceramics compared to conventional dental porcelains.

S Assmann1, M Ermrich, K Kunzmann.   

Abstract

In the present study, the leucite content of two different veneering porcelains and one pressable ceramic have been determined by X-ray diffraction after establishing a standard, using artificial leucite. The results are directly linked to the microstructure and mechanical properties of the materials. The most homogeneous glass-ceramic exhibits the highest relative leucite content and the highest fracture strength. Copyright 2000 Kluwer Academic Publishers

Entities:  

Year:  2000        PMID: 15348068     DOI: 10.1023/a:1008965831837

Source DB:  PubMed          Journal:  J Mater Sci Mater Med        ISSN: 0957-4530            Impact factor:   3.896


  8 in total

1.  Effect of cooling rate on leucite volume fraction in dental porcelains.

Authors:  J R Mackert; A L Evans
Journal:  J Dent Res       Date:  1991-02       Impact factor: 6.116

Review 2.  A review of all-ceramic restorations.

Authors:  M A Rosenblum; A Schulman
Journal:  J Am Dent Assoc       Date:  1997-03       Impact factor: 3.634

3.  Effect of cubic leucite stabilization on the flexural strength of feldspathic dental porcelain.

Authors:  I L Denry; J R Mackert; J A Holloway; S F Rosenstiel
Journal:  J Dent Res       Date:  1996-12       Impact factor: 6.116

4.  The effect of the leucite transformation on dental porcelain expansion.

Authors:  J R Mackert; M B Butts; C W Fairhurst
Journal:  Dent Mater       Date:  1986-02       Impact factor: 5.304

5.  [Use of x-ray diffraction for the mineralogical study of opaque ceramic-metallic dental porcelains].

Authors:  J Poggioli; J Tuleff
Journal:  Rev Fr Odontostomatol       Date:  1970-02

6.  Leucite content of selected dental porcelains.

Authors:  P W Piché; W J O'Brien; C L Groh; K M Boenke
Journal:  J Biomed Mater Res       Date:  1994-05

7.  Phase identification in dental porcelains for ceramo-metallic restorations.

Authors:  M M Barreiro; O Riesgo; E E Vicente
Journal:  Dent Mater       Date:  1989-01       Impact factor: 5.304

8.  [The chemical solubility and stability of low-melting dental porcelains].

Authors:  C Risito; H Lüthy; O Loeffel; P Schärer
Journal:  Schweiz Monatsschr Zahnmed       Date:  1995
  8 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.