Literature DB >> 15198391

Effects of filler size, water, and alcohol on hardness and laboratory wear of dental composites.

Justin I Schwartz1, Karl-Johan M Söderholm.   

Abstract

Three UEDMA/TEGDMA (50:50 by weight) based dental composites were made, each with filler loadings of 53 vol.%. The three composites contained silane-treated filler particles with average particle diameters of 1.5, 3.0, or 10.0 microm. Twelve specimens per composite were mounted on wear wheels and run through 200,000 cycles in an ACTA wear machine. Six of these specimens per material were worn in slurries consisting of 30 g ground Millet seed shells and 120 g ground rice mixed with 275 mL water. The remaining six specimens were worn in similar 25% ethanol-water slurries. The composite wear profiles were recorded with a profilometer and used to calculate the wear. Hardness values of the composites were also measured both before and after storage for 2 weeks in either water or in a 25% ethanol water solution. The wear and hardness values from the measurements were analyzed using ANOVA. The wear analysis showed that the finer composites (1.5 microm filler diameter) wore the least and the coarsest composites (10 microm filler diameter) the most. The wear was significantly higher in the ethanol water slurry than in the water slurry. The hardness value of the coarsest composite decreased more than the finest composite during storage in water or 25% ethanol water. The hardness decrease was most pronounced in the alcohol solution.

Entities:  

Mesh:

Substances:

Year:  2004        PMID: 15198391     DOI: 10.1080/00016350410005555

Source DB:  PubMed          Journal:  Acta Odontol Scand        ISSN: 0001-6357            Impact factor:   2.331


  6 in total

1.  Dental resin materials in vivo - TEM results after one year: a pilot study.

Authors:  Gerhard Gröger; Martin Rosentritt; Michael Behr; Josef Schröder; Gerhard Handel
Journal:  J Mater Sci Mater Med       Date:  2006-09       Impact factor: 3.896

2.  Nanohybrid vs. fine hybrid composite in extended class II cavities: 8-year results.

Authors:  Roland Frankenberger; Christian Reinelt; Norbert Krämer
Journal:  Clin Oral Investig       Date:  2013-03-23       Impact factor: 3.573

3.  The effect of aging on the mechanical properties of nanohybrid composites based on new monomer formulations.

Authors:  Christine Schmidt; Nicoleta Ilie
Journal:  Clin Oral Investig       Date:  2012-03-14       Impact factor: 3.573

4.  Influence of artificial aging: mechanical and physicochemical properties of dental composites under static and dynamic compression.

Authors:  P Ottl; M Warkentin; D C Gornig; R Maletz
Journal:  Clin Oral Investig       Date:  2021-08-28       Impact factor: 3.606

5.  Effects of air-polishing powders on color stability of composite resins.

Authors:  Ahmet Umut Güler; Ibrahim Duran; Ali Çağin Yücel; Pelin Ozkan
Journal:  J Appl Oral Sci       Date:  2011-07-22       Impact factor: 2.698

6.  Food Simulating Organic Solvents for Evaluating Crosslink Density of Bulk Fill Composite Resin.

Authors:  Neveen M Ayad; Hala A Bahgat; Eman Hussain Al Kaba; Maryam Hussain Buholayka
Journal:  Int J Dent       Date:  2017-04-12
  6 in total