The aim of this study was to analyze factors influencing the failures of tunnel restorations performed with a glass cermet cement (Ketac Silver). Caries activity, lesion size, tunnel cavity opening size, partial or total tunnel, composite lamination or operating time showed no significant correlation to failure rate. Twelve dentists in eight clinics clinically experienced and familiar with the tunnel technique placed 374 restorations. The occlusal sections of fifty percent of the restorations were laminated with hybrid resin composite. The results of the yearly clinical and radiographic evaluations over the course of 3 years were correlated to factors that could influence the failure rate using logistic regression analysis. At the 3-year recall a cumulative number of 305 restorations were available. The cumulative replacement rate was 20%. The main reasons for replacement were marginal ridge fracture (14%) and dentin caries (3%). Another 7% of the restorations which had not been replaced were classified as failures because of untreated dentin caries. The only significant variable observed was the individual failure rate of the participating dentists varying between 9 and 50% (p=0.013).Entities:
Mesh:
Substances:
Year: 2001 PMID: 11480816 DOI: 10.1007/s007840100106
Source DB: PubMed Journal: Clin Oral Investig ISSN: 1432-6981 Impact factor: 3.573