Resistance of two dentin-bonding agents and a dentin densensitizer to acid erosion in vitro.

P A Brunton1, K S Kalsi, D C Watts, N H Wilson.   

Abstract

OBJECTIVES: To determine the resistance of two dentin-bonding agents (DBAs) and a dentin desensitizer to simulated dental erosion.
METHODS: Twenty teeth in each of three groups of selected premolars, with exposed cervical dentin, were treated with one of three dentin surface treatment systems: Gluma Desensitizer (Heraeus Kulzer (UK) Ltd), One Coat Bond (Whaledent (UK) Ltd), and Optibond FL (Kerr (UK) Ltd) and exposed to water (control) and an erosive challenge (Coca Cola) for 14 days. Sequential tracings of the specimens were taken, superimposed and the mean reduction in densensitizer or DBA thickness and or tooth loss determined.
RESULTS: A mean loss of 77 microns (s.d. 14.6 microns) of tooth tissue over the untreated sites following 14 days exposure to Coca Cola was observed. The application of DBAs, as opposed to Gluma Desensistizer alone, over exposed dentin surfaces afforded substantial protection against erosion by Coca Cola over the period of study. The mean change in vertical profile of teeth treated with a DBA was 20 microns (s.d. 14.7 microns), almost four times less than that seen over untreated sites. SIGNIFICANCE: With the exception of Gluma Desensitizer, which was lost completely, One Coat Bond and Optibond FL demonstrated levels of acid dissolution resistance, which would be of potential value clinically.

Entities:  

Mesh:

Substances:

Year:  2000        PMID: 10915896     DOI: 10.1016/s0109-5641(00)00027-0

Source DB:  PubMed          Journal:  Dent Mater        ISSN: 0109-5641            Impact factor:   5.304


  7 in total

1.  Restoration variables and postoperative hypersensitivity in Class I restorations: PEARL Network findings. Part 2.

Authors:  Peter Blanchard; Ying Wong; Abigail G Matthews; Donald Vena; Ronald G Craig; Frederick A Curro; Van P Thompson
Journal:  Compend Contin Educ Dent       Date:  2013-04

Review 2.  Dental approach to erosive tooth wear in gastroesophageal reflux disease.

Authors:  Ayse Dundar; Abdulkadir Sengun
Journal:  Afr Health Sci       Date:  2014-06       Impact factor: 0.927

3.  Influence of light-curing mode on the erosion preventive effect of three different resin-based surface sealants.

Authors:  Florian J Wegehaupt; Tobias T Tauböck; Beatrice Sener; Thomas Attin
Journal:  Int J Dent       Date:  2012-09-06

4.  Long-term bonding to eroded dentin requires superficial bur preparation.

Authors:  Brigitte Zimmerli; Jan De Munck; Adrian Lussi; Paul Lambrechts; Bart Van Meerbeek
Journal:  Clin Oral Investig       Date:  2011-12-08       Impact factor: 3.573

5.  Long-Term Bond Strength of Two Benzalkonium Chloride-Modified Adhesive Systems to Eroded Dentin.

Authors:  Simon Flury; Adrian Lussi; Anne Peutzfeldt
Journal:  Biomed Res Int       Date:  2017-08-10       Impact factor: 3.411

6.  The Effect of SnCl2/AmF Pretreatment on Short- and Long-Term Bond Strength to Eroded Dentin.

Authors:  Katrin Zumstein; Anne Peutzfeldt; Adrian Lussi; Simon Flury
Journal:  Biomed Res Int       Date:  2018-04-19       Impact factor: 3.411

7.  Influence of light-curing mode on the cytotoxicity of resin-based surface sealants.

Authors:  Florian J Wegehaupt; Tobias T Tauböck; Thomas Attin; Georgios N Belibasakis
Journal:  BMC Oral Health       Date:  2014-05-06       Impact factor: 2.757

  7 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.