Tissue sensitivity to acrylic resin. A method of measuring the residual monomer content and its clinical application.

J F McCabe, R M Basker.   

Abstract

Entities:  

Mesh:

Substances:

Year:  1976        PMID: 1063578     DOI: 10.1038/sj.bdj.4803760

Source DB:  PubMed          Journal:  Br Dent J        ISSN: 0007-0610            Impact factor:   1.626


× No keyword cloud information.
  5 in total

1.  In Vitro Comparison of Compressive and Tensile Strengths ofAcrylic Resins Reinforced by Silver Nanoparticles at 2% and0.2% Concentrations.

Authors:  Tahereh Ghaffari; Fahimeh Hamedirad; Baharak Ezzati
Journal:  J Dent Res Dent Clin Dent Prospects       Date:  2014-12-03

2.  In vitro cytotoxicity of self-curing acrylic resins of different colors.

Authors:  Luciana Borges Retamoso; Taís de Morais Alves da Cunha; Matheus Melo Pithon; Rogério Lacerda dos Santos; Fernanda Otaviano Martins; Maria Teresa Villela Romanos; Orlando Motohiro Tanaka
Journal:  Dental Press J Orthod       Date:  2014 Jul-Aug

3.  Color stability, water sorption and cytotoxicity of thermoplastic acrylic resin for non metal clasp denture.

Authors:  Dae-Eun Jang; Ji-Young Lee; Hyun-Seon Jang; Jang-Jae Lee; Mee-Kyoung Son
Journal:  J Adv Prosthodont       Date:  2015-08-18       Impact factor: 1.904

4.  Effect of post-polymerization heat treatments on the cytotoxicity of two denture base acrylic resins.

Authors:  Janaina Habib Jorge; Eunice Teresinha Giampaolo; Carlos Eduardo Vergani; Ana Lúcia Machado; Ana Cláudia Pavarina; Iracilda Zeppone Carlos
Journal:  J Appl Oral Sci       Date:  2006-06       Impact factor: 2.698

5.  Management of dental trauma in a child with Xeroderma Pigmentosa.

Authors:  Nidhi Agarwal; Dipanshu Kumar; Aakansha Sharma; Ashish Anand
Journal:  Saudi Dent J       Date:  2017-09-23
  5 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.