Literature DB >> 9925564

Degradation of starch-poly(beta-hydroxybutyrate-co-beta-hydroxyvalerate) bioplastic in tropical coastal waters.

S H Imam1, S H Gordon, R L Shogren, T R Tosteson, N S Govind, R V Greene.   

Abstract

Extruded bioplastic was prepared from cornstarch or poly(beta-hydroxybutyrate-co-beta-hydroxyvalerate) (PHBV) or blends of cornstarch and PHBV. The blended formulations contained 30 or 50% starch in the presence or absence of polyethylene oxide (PEO), which enhances adherence of starch granules to PHBV. Degradation of these formulations was monitored for 1 year at four stations in coastal water southwest of Puerto Rico. Two stations were within a mangrove stand. The other two were offshore; one of these stations was on a shallow shoulder of a reef, and the other was at a location in deeper water. Microbial enumeration at the four stations revealed considerable flux in the populations over the course of the year. However, in general, the overall population densities were 1 order of magnitude less at the deeper-water station than at the other stations. Starch degraders were 10- to 50-fold more prevalent than PHBV degraders at all of the stations. Accordingly, degradation of the bioplastic, as determined by weight loss and deterioration of tensile properties, correlated with the amount of starch present (100% starch >50% starch > 30% starch > 100% PHBV). Incorporation of PEO into blends slightly retarded the rate of degradation. The rate of loss of starch from the 100% starch samples was about 2%/day, while the rate of loss of PHBV from the 100% PHBV samples was about 0.1%/day. Biphasic weight loss was observed for the starch-PHBV blends at all of the stations. A predictive mathematical model for loss of individual polymers from a 30% starch-70% PHBV formulation was developed and experimentally validated. The model showed that PHBV degradation was delayed 50 days until more than 80% of the starch was consumed and predicted that starch and PHBV in the blend had half-lives of 19 and 158 days, respectively. Consistent with the relatively low microbial populations, bioplastic degradation at the deeper-water station exhibited an initial lag period, after which degradation rates comparable to the degradation rates at the other stations were observed. Presumably, significant biodegradation occurred only after colonization of the plastic, a parameter that was dependent on the resident microbial populations. Therefore, it can be reasonably inferred that extended degradation lags would occur in open ocean water where microbes are sparse.

Entities:  

Mesh:

Substances:

Year:  1999        PMID: 9925564      PMCID: PMC91043     

Source DB:  PubMed          Journal:  Appl Environ Microbiol        ISSN: 0099-2240            Impact factor:   4.792


  4 in total

1.  Materials derived from biomass/biodegradable materials.

Authors:  W D Luzier
Journal:  Proc Natl Acad Sci U S A       Date:  1992-02-01       Impact factor: 11.205

2.  Growth characteristics of a novel nitrogen-fixing cellulolytic bacterium.

Authors:  R V Greene; S N Freer
Journal:  Appl Environ Microbiol       Date:  1986-11       Impact factor: 4.792

3.  Polymers for biodegradable medical devices. VI. Hydroxybutyrate-hydroxyvalerate copolymers: accelerated degradation of blends with polysaccharides.

Authors:  M Yasin; S J Holland; A M Jolly; B J Tighe
Journal:  Biomaterials       Date:  1989-08       Impact factor: 12.479

4.  Biodegradability and mechanical properties of poly-(beta-hydroxybutyrate-co-beta-hydroxyvalerate)-starch blends.

Authors:  B A Ramsay; V Langlade; P J Carreau; J A Ramsay
Journal:  Appl Environ Microbiol       Date:  1993-04       Impact factor: 4.792

  4 in total
  10 in total

1.  Bioplastic degradation in natural reservoirs differing in ecological parameters.

Authors:  O N Voinova; N A Kozhevnikova; M I Gladyshev; T G Volova
Journal:  Dokl Biol Sci       Date:  2007 Nov-Dec

Review 2.  Expanding Poly(lactic acid) (PLA) and Polyhydroxyalkanoates (PHAs) Applications: A Review on Modifications and Effects.

Authors:  Ahmed Z Naser; Ibrahim Deiab; Fantahun Defersha; Sheng Yang
Journal:  Polymers (Basel)       Date:  2021-12-06       Impact factor: 4.329

3.  Microbial Degradation of Polyhydroxyalkanoates with Different Chemical Compositions and Their Biodegradability.

Authors:  Tatiana G Volova; Svetlana V Prudnikova; Olga N Vinogradova; Darya A Syrvacheva; Ekaterina I Shishatskaya
Journal:  Microb Ecol       Date:  2016-09-13       Impact factor: 4.552

4.  Laboratory test methods to determine the degradation of plastics in marine environmental conditions.

Authors:  Maurizio Tosin; Miriam Weber; Michela Siotto; Christian Lott; Francesco Degli Innocenti
Journal:  Front Microbiol       Date:  2012-06-21       Impact factor: 5.640

5.  Ranking environmental degradation trends of plastic marine debris based on physical properties and molecular structure.

Authors:  Kyungjun Min; Joseph D Cuiffi; Robert T Mathers
Journal:  Nat Commun       Date:  2020-02-05       Impact factor: 14.919

6.  The effect of natural fillers on the marine biodegradation behaviour of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV).

Authors:  Kjeld W Meereboer; Akhilesh K Pal; Erick O Cisneros-López; Manjusri Misra; Amar K Mohanty
Journal:  Sci Rep       Date:  2021-01-13       Impact factor: 4.379

Review 7.  Seawater-Degradable Polymers-Fighting the Marine Plastic Pollution.

Authors:  Ge-Xia Wang; Dan Huang; Jun-Hui Ji; Carolin Völker; Frederik R Wurm
Journal:  Adv Sci (Weinh)       Date:  2020-11-23       Impact factor: 16.806

Review 8.  Biodegradability standards for carrier bags and plastic films in aquatic environments: a critical review.

Authors:  Jesse P Harrison; Carl Boardman; Kenneth O'Callaghan; Anne-Marie Delort; Jim Song
Journal:  R Soc Open Sci       Date:  2018-05-23       Impact factor: 2.963

9.  Novel Sustainable Composites Based on Poly(hydroxybutyrate-co-hydroxyvalerate) and Seagrass Beach-CAST Fibers: Performance and Degradability in Marine Environments.

Authors:  Maurizia Seggiani; Patrizia Cinelli; Elena Balestri; Norma Mallegni; Eleonora Stefanelli; Alessia Rossi; Claudio Lardicci; Andrea Lazzeri
Journal:  Materials (Basel)       Date:  2018-05-11       Impact factor: 3.623

10.  Field and mesocosm methods to test biodegradable plastic film under marine conditions.

Authors:  Christian Lott; Andreas Eich; Boris Unger; Dorothée Makarow; Glauco Battagliarin; Katharina Schlegel; Markus T Lasut; Miriam Weber
Journal:  PLoS One       Date:  2020-07-31       Impact factor: 3.240

  10 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.