A tough, thermally conductive silicon carbide composite with high strength up to 1600 degreesC in Air

.   

Abstract

A sintered silicon carbide fiber-bonded ceramic, which consists of a highly ordered, close-packed structure of very fine hexagonal columnar fibers with a thin interfacial carbon layer between fibers, was synthesized by hot-pressing plied sheets of an amorphous silicon-aluminum-carbon-oxygen fiber prepared from an organosilicon polymer. The interior of the fiber element was composed of sintered beta-silicon carbide crystal without an obvious second phase at the grain boundary and triple points. This material showed high strength (over 600 megapascals in longitudinal direction), fibrous fracture behavior, excellent high-temperature properties (up to 1600 degreesC in air), and high thermal conductivity (even at temperatures over 1000 degreesC).

Entities:  

Year:  1998        PMID: 9812889     DOI: 10.1126/science.282.5392.1295

Source DB:  PubMed          Journal:  Science        ISSN: 0036-8075            Impact factor:   47.728


  5 in total

1.  Effect of heat treatment on the microstructure and ablation performance of C/C-SiC composites containing ZrSi2-Si.

Authors:  Tianxing Jiang; Yi Zeng; Xiang Xiong; Ziming Ye; Huilin Lun; Shiyan Chen; Jinrun Hu; Ge Yang; Sen Gao
Journal:  RSC Adv       Date:  2021-05-07       Impact factor: 4.036

2.  Vertically Aligned Silicon Carbide Nanowires/Boron Nitride Cellulose Aerogel Networks Enhanced Thermal Conductivity and Electromagnetic Absorbing of Epoxy Composites.

Authors:  Duo Pan; Gui Yang; Hala M Abo-Dief; Jingwen Dong; Fengmei Su; Chuntai Liu; Yifan Li; Ben Bin Xu; Vignesh Murugadoss; Nithesh Naik; Salah M El-Bahy; Zeinhom M El-Bahy; Minan Huang; Zhanhu Guo
Journal:  Nanomicro Lett       Date:  2022-04-30

3.  Porous Silicon Oxycarbonitride Ceramics with Palladium and Pd2Si Nanoparticles for Dry Reforming of Methane.

Authors:  Jun Wang; Matthias Grünbacher; Simon Penner; Maged F Bekheet; Aleksander Gurlo
Journal:  Polymers (Basel)       Date:  2022-08-25       Impact factor: 4.967

4.  Ionization-induced annealing of pre-existing defects in silicon carbide.

Authors:  Yanwen Zhang; Ritesh Sachan; Olli H Pakarinen; Matthew F Chisholm; Peng Liu; Haizhou Xue; William J Weber
Journal:  Nat Commun       Date:  2015-08-12       Impact factor: 14.919

5.  Atomic Configuration of Point Defect Clusters in Ion-Irradiated Silicon Carbide.

Authors:  Y R Lin; L G Chen; C Y Hsieh; M T Chang; K Y Fung; A Hu; S C Lo; F R Chen; J J Kai
Journal:  Sci Rep       Date:  2017-11-07       Impact factor: 4.379

  5 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.