Effect of heat sterilization on the torsional properties of rotary nickel-titanium endodontic files.

J Silvaggio1, M L Hicks.   

Abstract

The purpose of this study was to determine whether heat sterilization adversely effects the torsional properties of rotary nickel-titanium files, making them more prone to fracture under torsional stress. Nine hundred sizes 2 through 10 Profile Series 29.04 taper files were divided into groups of 10 files each and sterilized 0, 1, 5, or 10 times in the steam autoclave, Statim autoclave, or dry heat sterilizer. Then, they were subjected to torsional testing in a Torquemeter Memocouple. Complete data were collected for sizes 2 through 7, but not for sizes 8 through 10 because their torque resistance exceeded the testing limits of the Torquemeter Memocouple. A one-way analysis of variance was used to compare all experimental groups in sizes 2 through 7 with their unsterilized controls (p < 0.05). Fifty-four comparisons were made for torsional strength and 54 for rotational flexibility. Ten significant changes occurred for torsional strength and 10 for rotational flexibility. Eight of 10 changes in torsional strength were increases. Fifty-two of 54 (96.3%) comparisons for torsional strength and 47 of 54 (87%) for rotational flexibility showed a significant increase or no change. Therefore, heat sterilization of rotary nickel-titanium files up to 10 times does not increase the likelihood of instrument fracture.

Entities:  

Mesh:

Substances:

Year:  1997        PMID: 9487847     DOI: 10.1016/S0099-2399(97)80344-5

Source DB:  PubMed          Journal:  J Endod        ISSN: 0099-2399            Impact factor:   4.171


  5 in total

1.  Effect of steam and dry heat sterilization on the insertion and fracture torque of orthodontic miniscrews.

Authors:  Shiva Alavi; Farnaz Asadi; Seyed Amir Hossein Raji; Soroor Samie
Journal:  Dent Res J (Isfahan)       Date:  2020-05-23

2.  Comparative evaluation of the effects of multiple autoclaving on cyclic fatigue resistance of three different rotary Ni-Ti instruments: An in vitro study.

Authors:  Kanthimathinathan Meenakshi Sundaram; Rajesh A V Ebenezar; Mohamed Fayas Ghani; Leena Martina; Ashwin Narayanan; Bejoy Mony
Journal:  J Conserv Dent       Date:  2013-07

3.  The Effect of Multiple Autoclave Sterilization on the Cyclic Fatigue of Three Heat-Treated Nickel-Titanium Rotary Files: EdgeFile X7, Vortex Blue, and TRUShape.

Authors:  Reham Sharroufna; Mohammed Mashyakhy
Journal:  Biomed Res Int       Date:  2020-12-14       Impact factor: 3.411

4.  Effect of autoclaving on the cyclic fatigue resistance of nickel-titanium rotary instruments: An in vitro study.

Authors:  Kukunuru Gayatri; Sravanthi Tammineedi; Nagesh Bolla; Sayesh Vemuri; Ram Chowdary Basam; Chukka Ram Sunil
Journal:  J Conserv Dent       Date:  2022-03-07

5.  Effect of Sterilization on Cyclic Fatigue Resistance of Proflexendo Endodontic Rotary Files.

Authors:  Emad O Alshwaimi
Journal:  Saudi J Med Med Sci       Date:  2019-02-08
  5 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.