Injection moulded hydroxyapatite ceramics.

J Cihlár1, M Trunec.   

Abstract

The injection moulding of hydroxyapatite (HA) and properties (relative density, shrinkage, microstructure, thermal strength and phase composition) of HA ceramics sintered at temperatures of 1373-1773 K were studied. Particles of oval shape and size of 0.5 microns were most suitable for injection moulding. Polymer/HA mixture contained 63 vol% of the HA powder. Maximum relative density (98.7%) and shrinkage (16%) of HA ceramics were obtained at a sintering temperature of 1523 K. Maximum flexural strength (60 MPa) of HA ceramics occurred at a sintering temperature of 1473 K. The strength of these ceramics decreased at sintering temperatures higher than 1473 K. Loss in strength was owing to the grain growth and decomposition of HA ceramics. The relationship between grain size and strength is described by the equation: sigma = 53.3d1/2. The calculated activation energy of grain growth obtained was 215kJ mol-1 K-1. The decomposition of HA to alpha-tricalcium phosphate was important at temperatures greater than 1573 K.

Entities:  

Mesh:

Substances:

Year:  1996        PMID: 8889072     DOI: 10.1016/0142-9612(95)00243-x

Source DB:  PubMed          Journal:  Biomaterials        ISSN: 0142-9612            Impact factor:   12.479


  5 in total

Review 1.  Calcium Orthophosphate-Based Bioceramics.

Authors:  Sergey V Dorozhkin
Journal:  Materials (Basel)       Date:  2013-09-06       Impact factor: 3.623

2.  Influence of temperature and aging time on HA synthesized by the hydrothermal method.

Authors:  C R Kothapalli; M Wei; R Z Legeros; M T Shaw
Journal:  J Mater Sci Mater Med       Date:  2005-05       Impact factor: 3.896

3.  Effect of vinyl acetate content on the sintering behavior of hydroxyapatite-ethylene vinyl acetate copolymer composites.

Authors:  Shiny Velayudhan; P Ramesh; H K Varma
Journal:  J Mater Sci Mater Med       Date:  2002-05       Impact factor: 3.896

4.  Injection Molding of 3-3 Hydroxyapatite Composites.

Authors:  Jonas Biggemann; Patrizia Hoffmann; Ivaylo Hristov; Swantje Simon; Philipp Müller; Tobias Fey
Journal:  Materials (Basel)       Date:  2020-04-17       Impact factor: 3.623

5.  Effect of sintering parameters on physical and mechanical properties of powder injection moulded stainless steel-hydroxyapatite composite.

Authors:  Mohd Ikram Ramli; Abu Bakar Sulong; Norhamidi Muhamad; Andanastuti Muchtar; Amir Arifin; Farhana Mohd Foudzi; Mohannad Saleh Hammadi Al-Furjan
Journal:  PLoS One       Date:  2018-10-25       Impact factor: 3.240

  5 in total