Literature DB >> 8380820

Comparative SEM and TEM examination of the ultrastructure of the resin-dentin interdiffusion zone.

B Van Meerbeek1, A Dhem, M Goret-Nicaise, M Braem, P Lambrechts, G VanHerle.   

Abstract

The resin-dentin interdiffusion zone produced by a dentin-adhesive system that removes the smear layer and concurrently decalcifies superficial dentin was morphologically examined by both scanning and transmission electron microscopy. Cross-sectioned resin-bonded dentin discs were etched with an argon-ion beam to make the resin-dentin interface observable by SEM. For the TEM examination, the sections were partly decalcified by an aqueous EDTA solution to facilitate ultramicrotomy and to disclose the ultrastructure of the interdiffusion zone. Both SEM and TEM confirmed the presence of the resin-dentin interdiffusion zone as the junction between the deep unaltered dentin structure and the restorative resin. Within the interdiffusion zone, three sublayers with characteristic ultrastructure and staining were identified by TEM. An upper diffuse black layer contained few structural features. Underneath, partially-altered collagen fibrils were closely packed, mostly running parallel with the interface and perpendicular to the dentinal tubules. Their outline was electron-dense, forming tunnel-like structures. At the base of the upper layer, several stained projections were found to bulge out into the underlying collagen network and appeared to be confined by obstructive, parallel-running collagen fibrils. Finally, the third dense layer, containing hydroxyapatite crystals, demarcated the superficially demineralized dentin layer from the deeper unaltered dentin. Resin diffusion into the decalcified dentin surface layer was evident, but diminished with depth, presumably reducing deeper resin impregnation into the interfibrillar spaces. The citric acid dentin-pretreatment probably caused denaturation of the superficial collagen fibrils. Its decalcifying effect gradually weakened with depth, leaving behind hydroxyapatite crystals at the base of the interdiffusion zone.(ABSTRACT TRUNCATED AT 250 WORDS)

Entities:  

Mesh:

Substances:

Year:  1993        PMID: 8380820     DOI: 10.1177/00220345930720020501

Source DB:  PubMed          Journal:  J Dent Res        ISSN: 0022-0345            Impact factor:   6.116


  23 in total

1.  Scanning acoustic microscopy investigation of frequency-dependent reflectance of acid- etched human dentin using homotopic measurements.

Authors:  Orestes Marangos; Anil Misra; Paulette Spencer; J Lawrence Katz
Journal:  IEEE Trans Ultrason Ferroelectr Freq Control       Date:  2011-03       Impact factor: 2.725

2.  Analysis of surfaces and adhesive interfaces of enamel and dentin after different treatments.

Authors:  Michelle Alexandra Chinelatti; Silmara Aparecida Milori Corona; Maria Cristina Borsatto; Lilian Faria Ribeiro; Renata Andréa Salvitti de Sá Rocha; Regina Guenka Palma-Dibb
Journal:  J Mater Sci Mater Med       Date:  2007-03-27       Impact factor: 3.896

Review 3.  Classification review of dental adhesive systems: from the IV generation to the universal type.

Authors:  Eshrak Sofan; Afrah Sofan; Gaspare Palaia; Gianluca Tenore; Umberto Romeo; Guido Migliau
Journal:  Ann Stomatol (Roma)       Date:  2017-07-03

4.  Non-thermal atmospheric plasma brush induces HEMA grafting onto dentin collagen.

Authors:  Mingsheng Chen; Ying Zhang; Vladimir Dusevich; Yi Liu; Qingsong Yu; Yong Wang
Journal:  Dent Mater       Date:  2014-11-11       Impact factor: 5.304

5.  Resin-dentin bonding interface after photochemical surface treatment.

Authors:  Ken-ichi Tonami; Kazunobu Sano; Shizuko Ichinose; Kouji Araki
Journal:  Photomed Laser Surg       Date:  2015-01-02       Impact factor: 2.796

Review 6.  Optimizing dentin bond durability: control of collagen degradation by matrix metalloproteinases and cysteine cathepsins.

Authors:  Leo Tjäderhane; Fabio D Nascimento; Lorenzo Breschi; Annalisa Mazzoni; Ivarne L S Tersariol; Saulo Geraldeli; Arzu Tezvergil-Mutluay; Marcela R Carrilho; Ricardo M Carvalho; Franklin R Tay; David H Pashley
Journal:  Dent Mater       Date:  2012-08-16       Impact factor: 5.304

7.  Two-photon laser confocal microscopy of micropermeability of resin-dentin bonds made with water or ethanol wet bonding.

Authors:  Salvatore Sauro; Timothy F Watson; Francesco Mannocci; Katsuya Miyake; Bradford P Huffman; Franklin R Tay; David H Pashley
Journal:  J Biomed Mater Res B Appl Biomater       Date:  2009-07       Impact factor: 3.368

8.  The use of collagen cross-linking agents to enhance dentin bond strength.

Authors:  Aiman Al-Ammar; James L Drummond; Ana Karina Bedran-Russo
Journal:  J Biomed Mater Res B Appl Biomater       Date:  2009-10       Impact factor: 3.368

9.  A rapid nondestructive method for root dentin moisture measurements: in vitro pilot study.

Authors:  Takashi Komabayashi; Qiang Zhu; Jin Jiang; Kamran E Safavi; Larz S W Spångberg
Journal:  Oral Surg Oral Med Oral Pathol Oral Radiol Endod       Date:  2009-01-20

10.  Microleakage and Resin-to-Dentin Interface Morphology of Pre-Etching versus Self-Etching Adhesive Systems.

Authors:  G L Waldman; T K Vaidyanathan; J Vaidyanathan
Journal:  Open Dent J       Date:  2008-11-28
View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.