Effects of treatment and storage conditions on ceramic/composite bond strength.

J F Roulet1, K J Söderholm, J Longmate.   

Abstract

During the past few years, the interest in using ceramic inlays and veneers has increased. New materials and methods have been introduced to bond these restorations to resinous materials. Since our knowledge of how to optimize such bonding is limited, the objective of this study was to test the hypothesis that various surface treatment variables and combinations of these variables affect the strength of the ceramic/composite interphase of ceramic inlays differently. The influences of material composition, surface-roughening method, silane treatment, silane heat treatment, and storage condition on bond strength were investigated. Three ceramics (Dicor, Mirage, Vitabloc), three surface-roughening methods (etching, sandblasting, grinding), three silane treatments (gamma-methacryloxypropyltrimethoxysilane [MPS], MPS+paratoluidine, vinyltrichlorosilane), two heat treatments (20 degrees C for 60 s, 100 degrees C for 60 s), and two storage conditions (24-hour dry, one yr in water at 37 degrees C) were studied. For each of the 108 combinations, five specimens were tested. Ceramic cylinders were treated according to group assignment and bonded to blocks of the same ceramic material with a dual-cured resin. The shear bond strength was determined, and the experimental factors were evaluated by analysis of variance. The results showed that surface-roughening method had the strongest effect on bond strength, while ceramic selection had the least significant effect. Of the surface-roughening methods, etching was associated with higher bond strength values than either sandblasting or grinding.(ABSTRACT TRUNCATED AT 250 WORDS)

Entities:  

Mesh:

Substances:

Year:  1995        PMID: 7876433     DOI: 10.1177/00220345950740011501

Source DB:  PubMed          Journal:  J Dent Res        ISSN: 0022-0345            Impact factor:   6.116


  18 in total

1.  Bond strength of composite resin to glass ceramic after saliva contamination.

Authors:  Frank Nikolaus; Martin Wolkewitz; Petra Hahn
Journal:  Clin Oral Investig       Date:  2012-06-23       Impact factor: 3.573

2.  Effect of different surface treatments on the composite-composite repair bond strength.

Authors:  Andreas Rathke; Yana Tymina; Bernd Haller
Journal:  Clin Oral Investig       Date:  2008-10-07       Impact factor: 3.573

3.  Immediate bonding effectiveness of contemporary composite cements to dentin.

Authors:  Mouhamed Sarr; Atsushi Mine; Jan De Munck; Marcio Vivan Cardoso; Abdoul Wakhabe Kane; José Vreven; Bart Van Meerbeek; Kirsten L Van Landuyt
Journal:  Clin Oral Investig       Date:  2009-08-25       Impact factor: 3.573

4.  Microtensile bond strength of self-adhesive luting cements to ceramics.

Authors:  Tomoko Abo; Shigeru Uno; Masahiro Yoshiyama; Toshimoto Yamada; Nobuhiro Hanada
Journal:  Int J Dent       Date:  2012-04-23

5.  Effect of surface treatment with laser on repair bond strength of composite resin to ceramic.

Authors:  Nazanin Kiomarsi; Azin Jarrah; Nasim Chiniforoush; Sedighe Sadat Hashemikamangar; Mohammad Javad Kharazifard
Journal:  Dent Res J (Isfahan)       Date:  2022-03-21

6.  Use of zinc phosphate cement as a luting agent for Denzir trade mark copings: an in vitro study.

Authors:  Karl-Johan M Söderholm; Eduardo Mondragon; Ileana Garcea
Journal:  BMC Oral Health       Date:  2003-02-07       Impact factor: 2.757

7.  Tensile bond strength of four denture resins to porcelain teeth with different surface treatment.

Authors:  Mohamed El-Sheikh; John Powers
Journal:  J Adv Prosthodont       Date:  2013-11-28       Impact factor: 1.904

8.  How will surface treatments affect the translucency of porcelain laminate veneers?

Authors:  Sedanur Turgut; Bora Bagis; Elif Aydogan Ayaz; Fatih Mehmet Korkmaz; Kıvanç Utku Ulusoy; Yildirim Hakan Bagis
Journal:  J Adv Prosthodont       Date:  2014-02-14       Impact factor: 1.904

9.  Shear Bond Strength of Repaired Composites Using Surface Treatments and Repair Materials: An In vitro Study.

Authors:  M Hemadri; G Saritha; V Rajasekhar; K Amit Pachlag; R Purushotham; Veera Kishore Kumar Reddy
Journal:  J Int Oral Health       Date:  2014 Nov-Dec

10.  Silane Heat Treatment Could Eliminate the Hydrofluoric Acid Etching of Lithium Disilicate Overlays: A Four-Year Follow-Up.

Authors:  Spartak Spasov Yanakiev; Mirela Borislavova Marinova-Takorova
Journal:  Case Rep Dent       Date:  2021-06-22
View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.