The mechanical properties of milled and cast titanium for ceramic veneering.

A W King1, J Chai, E Lautenschlager, J Gilbert.   

Abstract

This study compared the mechanical properties of machine-milled pure titanium and cast titanium. The metals were cast or milled to the dimensions of a standard tensile bar pattern. Each group was treated under three different conditions: as-cast (or as-milled), standard heat, and extended heat. Tensile testing found no difference in the mechanical properties of as-cast and as-milled titanium. Heat treatment significantly increased the ultimate tensile strength and the yield strength of cast titanium but had no such effects on milled titanium. There was no significant difference between the two metals in the modulus of elasticity or the percentage of elongation under the three treatment conditions.

Entities:  

Mesh:

Substances:

Year:  1994        PMID: 7748447

Source DB:  PubMed          Journal:  Int J Prosthodont        ISSN: 0893-2174            Impact factor:   1.681


  1 in total

Review 1.  Effects of Wire EDM on the Microstructure of P/M Titanium Samples.

Authors:  Joško Viskić; Zdravko Schauperl; Amir Ćatić; Martin Balog; Peter Krizik; Biserka Gržeta; Jasminka Popović; Slađana Milardović Ortolan; Ketij Mehulić
Journal:  Acta Stomatol Croat       Date:  2014-12
  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.