[Bonding strength between porcelain and gold alloys. (2) The effects of iron, indium and tin (author's transl)].

H Iwama, K Nakamura.   

Abstract

Ten kinds of alloys were prepared for testing by addition of 0-0.75 wt% iron, indium and tin (total amount 0.75 wt%) to base alloy, 88 Au-6 Pt-5 Pd-1 Ag. Opaque porcelain (Ceramco Inc.) was fused to these alloys according to the manufacturer's directions. The bonding strength was determined by the shear bond test that had been described in the preceding paper and the effects of the trace elements were examined.

Entities:  

Mesh:

Substances:

Year:  1976        PMID: 772140

Source DB:  PubMed          Journal:  Shika Rikogaku Zasshi        ISSN: 0583-0273


  1 in total

1.  A Comparison between Shear Bond Strength of VMK Master Porcelain with Three Base-metal Alloys (Ni-cr-T3, VeraBond, Super Cast) and One Noble Alloy (X-33) in Metal-ceramic Restorations.

Authors:  A Ahmadzadeh; A Neshati; N Mousavi; S Epakchi; F Dabaghi Tabriz; Ah Sarbazi
Journal:  J Dent (Shiraz)       Date:  2013-12
  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.