K Kawai1, M Hayashi, M Torii, Y Tsuchitani.
Abstract
The authors investigated the marginal adaptation and internal fit of ceramic inlay made by a ceramic milling system. The study's results indicated that the mean marginal and internal gap size of the ceramic inlay restorations was less than 100 microns, making the fit clinically acceptable.Mesh:
Substances:
Year: 1995 PMID: 7594014 DOI: 10.14219/jada.archive.1995.0053