Literature DB >> 6991561

Bonding of polymers to enamel: influence of deposits formed during etching, etching time and period of water immersion.

D R Beech, T Jalaly.   

Abstract

A technique for measuring the shear bond strength of composites to etched enamel was developed. The importance of thorough washing of the enamel surface to remove deposits formed during etching was demonstrated by measurements of bond strength and by scanning electron microscopy. One of three orthodontic adhesive systems showed a highly significant increase in bond strength after immersion in water for three months. Etching times as short as five seconds gave a bond strength not significantly different from that obtained after a one-minute etch.

Entities:  

Mesh:

Substances:

Year:  1980        PMID: 6991561     DOI: 10.1177/00220345800590071101

Source DB:  PubMed          Journal:  J Dent Res        ISSN: 0022-0345            Impact factor:   6.116


  6 in total

1.  [Reduced preliminary acid treatment of enamel in the bracket adhesion technic--a scanning electron microscopy and physical study].

Authors:  J Weissenberg; P Diedrich
Journal:  Fortschr Kieferorthop       Date:  1988-02

2.  Characterization of the porosity of human dental enamel and shear bond strength in vitro after variable etch times: initial findings using the BET method.

Authors:  Trang T Nguyen; Arthur Miller; Maria F Orellana
Journal:  Angle Orthod       Date:  2011-02-21       Impact factor: 2.079

3.  Evaluation of developmentally hypomineralised enamel after surface pretreatment with Papacarie Duo gel and different etching modes: an in vitro SEM and AFM study.

Authors:  Y-L Lee; K C Li; C K Y Yiu; D H Boyd; M Ekambaram
Journal:  Eur Arch Paediatr Dent       Date:  2021-09-29

4.  The effect of using different rinsing angles on the micro-tensile bond strength of the sealant to the etched enamel.

Authors:  Hossein Afshar; Yahya Baradaran Nakhajavani; Rahil Ahmadi
Journal:  Contemp Clin Dent       Date:  2013-04

5.  Temperature Rise Induced by Light Curing Unit Can Shorten Enamel Acid-Etching Time.

Authors:  Ahmad Najafi Abrandabadi; Seyedeh Mahsa Sheikh-Al-Eslamian; Narges Panahandeh
Journal:  J Dent (Tehran)       Date:  2015-12

6.  The effect of using different rinsing angles on the micro-tensile bond strength of the sealant to the etched enamel.

Authors:  Hossein Afshar; Yahya Baradaran Nakhjavani; Rahil Ahmadi
Journal:  Contemp Clin Dent       Date:  2014-01
  6 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.