Literature DB >> 6273445

The in-vitro degradation of poly(glycolic acid) sutures--effect of pH.

C C Chu.   

Abstract

Tensile strength of poly(glycolic acid) suture (PGA) of size 2-0 was examined as a function of three pH levels, 5.25, 7.44, and 10.09 of the buffer. Cord and yarn grip was used to eliminate grip-induced failure of breaking strength tests. It was found that Dexon sutures degraded significantly faster in pH = 10.09 buffer than the other two lower pH buffers. There was no significant difference in degradation rate at pH = 5.25 and 7.44. At 7 days, PGA sutures lost almost half of its original tensile strength at pH = 10.09, while the same sutures still remained more than 95% of their original breaking strength at buffers of pH = 5.25 and 7.44. After 21 days, no trace of sutures could be detected in the buffer of pH = 10.09 while about 20% strength still remained in the buffers of pH = 7.44 and 5.25. Cage effect in the crystalline phase and pH dependent hydrogen bonding were introduced to explain the difference in degradation phenomenon of PGA at buffers of various pH.

Entities:  

Mesh:

Substances:

Year:  1981        PMID: 6273445     DOI: 10.1002/jbm.820150604

Source DB:  PubMed          Journal:  J Biomed Mater Res        ISSN: 0021-9304


  9 in total

1.  PLGA/Ag nanocomposites: in vitro degradation study and silver ion release.

Authors:  E Fortunati; L Latterini; S Rinaldi; J M Kenny; I Armentano
Journal:  J Mater Sci Mater Med       Date:  2011-10-15       Impact factor: 3.896

Review 2.  Fabrication and Plasma Modification of Nanofibrous Tissue Engineering Scaffolds.

Authors:  Mahtab Asadian; Ke Vin Chan; Mohammad Norouzi; Silvia Grande; Pieter Cools; Rino Morent; Nathalie De Geyter
Journal:  Nanomaterials (Basel)       Date:  2020-01-08       Impact factor: 5.076

3.  An in vitro evaluation of the stability of mechanical properties of surgical suture materials in various pH conditions.

Authors:  C C Chu; G Moncrief
Journal:  Ann Surg       Date:  1983-08       Impact factor: 12.969

4.  Highly elastomeric poly(glycerol sebacate)-co-poly(ethylene glycol) amphiphilic block copolymers.

Authors:  Alpesh Patel; Akhilesh K Gaharwar; Giorgio Iviglia; Hongbin Zhang; Shilpaa Mukundan; Silvia M Mihaila; Danilo Demarchi; Ali Khademhosseini
Journal:  Biomaterials       Date:  2013-03-01       Impact factor: 12.479

5.  Mechanical properties of biodegradable polymer sutures coated with bioactive glass.

Authors:  A Stamboulis; L L Hench; A R Boccaccini
Journal:  J Mater Sci Mater Med       Date:  2002-09       Impact factor: 3.896

6.  Polyglycolide: degradation and drug release. Part I: changes in morphology during degradation.

Authors:  S Hurrell; R E Cameron
Journal:  J Mater Sci Mater Med       Date:  2001-09       Impact factor: 3.896

7.  The use of chitin as a new absorbable suture material--an experimental study.

Authors:  M Tachibana; A Yaita; H Taniura; K Fukasawa; N Nagasue; T Nakamura
Journal:  Jpn J Surg       Date:  1988-09

8.  X-ray phase-contrast computed tomography visualizes the microstructure and degradation profile of implanted biodegradable scaffolds after spinal cord injury.

Authors:  Kenta Takashima; Masato Hoshino; Kentaro Uesugi; Naoto Yagi; Shojiro Matsuda; Atsushi Nakahira; Noriko Osumi; Masahiro Kohzuki; Hiroshi Onodera
Journal:  J Synchrotron Radiat       Date:  2015-01-01       Impact factor: 2.616

9.  Effect on the tensile strength of human acellular dermis (Epiflex®) of in-vitro incubation simulating an open abdomen setting.

Authors:  Mario Vitacolonna; Michael Mularczyk; Florian Herrle; Torsten J Schulze; Hans Haupt; Matthias Oechsner; Lothar R Pilz; Peter Hohenberger; Eric Dominic Rössner
Journal:  BMC Surg       Date:  2014-01-27       Impact factor: 2.102

  9 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.