Literature DB >> 429383

In vitro corrosion of Ti-6Al-4V and type 316L stainless steel when galvanically coupled with carbon.

N G Thompson, R A Buchanan, J E Lemons.   

Abstract

In vitro corrosion experiments were conducted employing potentiostatic polarization techniques, a saline environment and candidate biomaterial alloy/carbon combinations. Corrosion currents and potentials of carbon/metal couples were predicted by mixed-potential theory utilizing the polarization curves generated. The alloys examined were annealed ELI grade Ti-6A1-4V and cold-worked 316L stainless steel while the types of carbon examined were LTI pyrolytic carbon and vapor-deposited carbon. It was determined that galvanic couples of carbon to cold-worked 316L stainless steel with carbon/metal area ratios of 10:1 to 100:1 produced coupled corrosion potentials in the range of the observed breakdown potential of the stainless steel. It was therefore predicted that localized corrosion in the form of pitting could occur on the cold-worked stainless steel when coupled to carbon with area ratios of 10:1 or greater. The titanium alloy did not exhibit a breakdown potential up to a potential of 1.2 V. Therefore, accelerated corrosion was not predicted for the titanium alloy to carbon galvanic couples under these experimental conditions. Direct carbon/alloy coupling experiments were conducted to verify the corrosion currents and potentials predicted from mixed-potential theory and polarization curve analysis. The experimental and theoretical values showed good agreement.

Entities:  

Mesh:

Substances:

Year:  1979        PMID: 429383     DOI: 10.1002/jbm.820130106

Source DB:  PubMed          Journal:  J Biomed Mater Res        ISSN: 0021-9304


  3 in total

1.  In vitro biocompatibility and corrosion resistance of a new implant titanium base alloy.

Authors:  E Vasilescu; P Drob; D Raducanu; V D Cojocaru; I Cinca; D Iordachescu; R Ion; M Popa; C Vasilescu
Journal:  J Mater Sci Mater Med       Date:  2010-03-25       Impact factor: 3.896

2.  Long-term assessment of the implant titanium material--artificial saliva interface.

Authors:  M V Popa; E Vasilescu; P Drob; C Vasilescu; I Demetrescu; D Ionita
Journal:  J Mater Sci Mater Med       Date:  2007-11-08       Impact factor: 3.896

Review 3.  Corrosion degradation and prevention by surface modification of biometallic materials.

Authors:  Raghuvir Singh; Narendra B Dahotre
Journal:  J Mater Sci Mater Med       Date:  2006-12-02       Impact factor: 4.727

  3 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.