Bonding of dental porcelain to ceramic-metal alloys.

E K Uusalo, V P Lassila, A U Yli-Urpo.   

Abstract

The bond strength of porcelain to the four gold alloys and the three nonprecious alloys was tested with a simplified pull test method, having wide test surfaces. The tests showed that all gold alloys tested were suitable for fusing porcelain. The bond strength in nonprecious alloys was somewhat lower and the location of the fracture lines was more variable. It seems that nonprecious alloys are more sensitive to laboratory procedures. The bond strength and the location of the fracture line had a good correlation in all metal alloys.

Entities:  

Mesh:

Substances:

Year:  1987        PMID: 3543308     DOI: 10.1016/0022-3913(87)90111-9

Source DB:  PubMed          Journal:  J Prosthet Dent        ISSN: 0022-3913            Impact factor:   3.426


  4 in total

1.  Surface bond strength in nickel based alloys.

Authors:  Ganesh Ramesh; T V Padmanabhan; Padma Ariga; Shalini Joshi; S Bhuminathan; Vasantha Vijayaraghavan
Journal:  J Indian Prosthodont Soc       Date:  2012-10-06

2.  Evaluation and comparison of shear bond strength of porcelain to a beryllium-free alloy of nickel-chromium, nickel and beryllium free alloy of cobalt-chromium, and titanium: An in vitro study.

Authors:  Ananya Singh; Keerthi Ramachandra; Achut R Devarhubli
Journal:  J Indian Prosthodont Soc       Date:  2017 Jul-Sep

3.  "Effect of Palatal Metal Collar's Height on Fracture Resistance of Single Metal-Ceramic Crowns".

Authors:  Nour Aburaisi; Haitham Elbishari
Journal:  Int J Dent       Date:  2022-10-07

4.  Bond and fracture strength of metal-ceramic restorations formed by selective laser sintering.

Authors:  Eun-Jeong Bae; Ji-Hwan Kim; Woong-Chul Kim; Hae-Young Kim
Journal:  J Adv Prosthodont       Date:  2014-08-14       Impact factor: 1.904

  4 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.