Bonding strengths of etched porcelain discs and three different bonding agents.

J G Lee, B K Moore, D R Avery, S T Hovijitra.   

Abstract

Forty porcelain disks were resin bonded to etched base metal surfaces to measure tensile bond strengths. One metal surface was bonded to each porcelain surface, making each test specimen "sandwiched", with a porcelain disk between two metal surfaces. The mean bond strength values of the Conclude group was 3017 +/- 869 psi. The mean for the Mar-Bond group was 3747 +/- 693 psi, and the mean for the two Chameleon groups combined was 3172 +/- 544 psi. No two groups were significantly different.

Entities:  

Mesh:

Substances:

Year:  1986        PMID: 3540045

Source DB:  PubMed          Journal:  ASDC J Dent Child        ISSN: 1945-1954


  1 in total

1.  In-vitro study of the adhesive strengths of brackets on metals, ceramic and composite. Part 2: Bonding to porcelain and composite resin.

Authors:  P G Jost-Brinkmann; S Can; C Drost
Journal:  J Orofac Orthop       Date:  1996-06       Impact factor: 1.938

  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.