Comparison of the strengths of aluminous porcelain fired on to platinum and palladium foils.

V Piddock, P M Marquis, H J Wilson.   

Abstract

The disc strengths of aluminous porcelain fired on to both platinum and palladium foil matrices have been determined. Also, the effect on strength of removing the matrices has been measured. The appearance of the separated metal and porcelain surfaces has been studied using scanning electron microscopy, and energy dispersive X-ray analysis has been used to evaluate the chemical composition of these surfaces. Reasons for the increase in strength observed when the matrix is left intact are discussed. Practical suggestions for obtaining stronger jacket crowns are presented.

Entities:  

Mesh:

Substances:

Year:  1986        PMID: 3511196     DOI: 10.1111/j.1365-2842.1986.tb01553.x

Source DB:  PubMed          Journal:  J Oral Rehabil        ISSN: 0305-182X            Impact factor:   3.837


  2 in total

1.  The effect of ZrO2 and TiO 2 on solubility and strength of apatite-mullite glass-ceramics for dental applications.

Authors:  Hawa M Fathi; Cheryl Miller; Christopher Stokes; Anthony Johnson
Journal:  J Mater Sci Mater Med       Date:  2013-11-19       Impact factor: 3.896

2.  Denture Base Composites: Effect of Surface Modified Nano- and Micro-Particulates on Mechanical Properties of Polymethyl Methacrylate.

Authors:  Touraj Nejatian; Neil Nathwani; Louise Taylor; Farshid Sefat
Journal:  Materials (Basel)       Date:  2020-01-09       Impact factor: 3.623

  2 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.