Literature DB >> 34372104

Optimum Preparation Conditions for Highly Individualized Chitin Nanofibers Using Ultrasonic Generator.

Dagmawi Abebe Zewude1, Hironori Izawa1,2, Shinsuke Ifuku1,2.   

Abstract

α-Chitin derived from crab shells was treated with 30% sodium hydroxide to prepare partially deacetylated chitin with a deacetylation degree of 36%. Partially deacetylated chitin nanofibers were prepared by applying weak ultrasonic energy generated by a domestic ultrasonic cleaner. The deacetylated chitin was easily disintegrated into nanofibers with the aid of electrostatic repulsion and osmotic pressure effect of amino cations on the chitin surfaces. The nanofibers were characterized in terms of yield, morphology, crystallinity, viscosity, and dispersibility. After a series of characterizations, ultrasonication with 45 kHz frequency and 20 min treatment was found to be the optimum conditions for obtaining fine nanofibers with a high yield.

Entities:  

Keywords:  nanofiber; partial deacetylation; ultrasonic treatment

Year:  2021        PMID: 34372104     DOI: 10.3390/polym13152501

Source DB:  PubMed          Journal:  Polymers (Basel)        ISSN: 2073-4360            Impact factor:   4.329


  1 in total

1.  Polyaniline-Grafted Chitin Nanocrystals as Conductive Reinforcing Nanofillers for Waterborne Polymer Dispersions.

Authors:  Emna Ben Ayed; Nouha Ghorbel; Ali Kallel; Jean-Luc Putaux; Sami Boufi
Journal:  Biomacromolecules       Date:  2022-09-08       Impact factor: 6.978

  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.