Ultraviolet Luminescence of ZnO Whiskers, Nanowalls, Multipods, and Ceramics as Potential Materials for Fast Scintillators.

Ivan D Venevtsev1, Andrey P Tarasov2, Arsen E Muslimov2, Elena I Gorokhova3, Ludmila A Zadorozhnaya2, Piotr A Rodnyi1, Vladimir M Kanevsky2.   

Abstract

The presented work is dedicated to the study and comparison of scintillating properties of zinc oxide samples prepared in different morphologies: whiskers, nanowalls, multipods, and ceramics. It was shown that total transmittance, photo- and radioluminescence spectra, and radioluminescence kinetics can vary significantly depending on sample structure and preparation conditions. The highest total transmittance was registered for ZnO ceramics (>50% at 0.5 mm thickness). Differences in the transmittance of whiskers, nanowalls, and multipods can be attributed to their shape and thickness which affects the amount of light refraction and scattering. The study of radioluminescence demonstrated that all samples, except undoped ceramics and air annealed whiskers, have predominantly fast luminescence with a decay time <1 ns. High transmittance of ceramics opens the way for their use in the registration of high energy X-ray and gamma radiation, where a large volume of scintillators is required. In cases, where large scintillator thickness is not a necessity, one may prefer to use other ZnO structures, such as ensembles of whiskers and nanowalls. Studies of near-band-edge luminescence components at low temperatures showed that the structure is quite similar in all samples except Ga doped ceramics.

Entities:  

Keywords:  X-ray induced luminescence; ceramics; fast scintillators; multipods; nanowalls; near-band-edge luminescence; photoluminescence; radioluminescence; total optical transmittance; whiskers; zinc oxide

Year:  2021        PMID: 33923610     DOI: 10.3390/ma14082001

Source DB:  PubMed          Journal:  Materials (Basel)        ISSN: 1996-1944            Impact factor:   3.623


  2 in total

1.  Positive Effects of a Perovskite Film on the Radioluminescence Properties of a ZnO:Ga Crystal Scintillator.

Authors:  Shiyi He; Yang Li; Liang Chen; Tong Jin; Linyue Liu; Jinlu Ruan; Xiaoping Ouyang
Journal:  Materials (Basel)       Date:  2022-02-16       Impact factor: 3.623

2.  Free-Standing ZnO:Mo Nanorods Exposed to Hydrogen or Oxygen Plasma: Influence on the Intrinsic and Extrinsic Defect States.

Authors:  Maksym Buryi; Zdeněk Remeš; Vladimir Babin; Sergii Chertopalov; Kateřina Děcká; Filip Dominec; Júlia Mičová; Neda Neykova
Journal:  Materials (Basel)       Date:  2022-03-18       Impact factor: 3.623

  2 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.