Mechanical Properties and Metal-Ceramic Bond Strength of Co-Cr Alloy Manufactured by Selective Laser Melting.

Joon-Ki Hong1, Seong-Kyun Kim1, Seong-Joo Heo1, Jai-Young Koak1.   

Abstract

Cobalt-chromium (Co-Cr) metal is one of the widely used biomaterials in the fabrication of dental prosthesis. The purpose of this study was to investigate whether there are differences in the properties of metals and bond strength with ceramics depending on the manufacturing methods of Co-Cr alloy. Co-Cr alloy specimens were prepared in three different ways: casting, milling, and selective laser melting (SLM). The mechanical properties (elastic modulus, yield strength, and flexural strength) of the alloys were investigated by flexure method in three-point bending mode, and microstructures of the specimens were analyzed. After application of the veneering ceramic through the three-point bending test, bond strength of the Metal-Ceramic was investigated. The cracked surfaces were observed by means of energy dispersive X-ray (EDX) spectroscopy and scanning electron microscopy (SEM) with backscattered electron (BSE) images. In mechanical properties, the elastic modulus was highest for the casting group, and the yield strength and flexural strength were lowest for the milling group. The SLM group showed finer homogeneous crystalline-microstructure, and a layered structure was observed at the fractured surface. After the ceramic bond strength test, all groups showed a mixed failure pattern. The casting group showed the highest bond strengths, whereas there was no significant difference between the other two groups. However, all groups have met the standard of bond strength according to international standards organization (ISO) with the appropriate passing rate. The results of this study indicate that the SLM manufacturing method may have the potential to replace traditional techniques for fabricating dental prosthesis.

Entities:  

Keywords:  3D printing; Co-Cr alloy; Metal-Ceramic bond strength; mechanical properties; selective laser melting

Year:  2020        PMID: 33339320     DOI: 10.3390/ma13245745

Source DB:  PubMed          Journal:  Materials (Basel)        ISSN: 1996-1944            Impact factor:   3.623


  2 in total

1.  Characterization of Co-Cr-W Dental Alloys with Veneering Materials Manufactured via Subtractive Milling and Additive Manufacturing LDED Methods.

Authors:  Óscar Barro; Felipe Arias-González; Fernando Lusquiños; Rafael Comesaña; Jesús Del Val; Antonio Riveiro; Aida Badaoui; Félix Gómez-Baño; Juan Pou
Journal:  Materials (Basel)       Date:  2022-06-30       Impact factor: 3.748

2.  An In Vitro Study on the Shear Bond Strength of Feldspathic Porcelain to Nickel Chromium Alloy and Cobalt Chromium Alloy after Various Surface Treatments.

Authors:  Vignesh Kamath; Mayuri Kamath; Abhinav Bhargava; Thilak Shetty; Shobha J Rodrigues; Umesh Y Pai; Sharon Saldanha; M Mahesh; Puneeth Hegde; Prashant Bajantri; Sandipan Mukherjee; Ann Sales
Journal:  Int J Dent       Date:  2022-05-30
  2 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.