The Mechanical Performance of a Novel Self-Adhesive Restorative Material.

Ulrich Lohbauer, Renan Belli.   

Abstract

PURPOSE: The development of a novel material requires a comprehensive pre-clinical assessment of clinical longevity before any market release. This study aimed to investigate the mechanical performance of a novel self-adhesive restorative material (ASAR MP4).
MATERIALS AND METHODS: Fracture strength (FS), flexural fatigue strength (FFS) and fracture toughness (KIc) were measured for the experimental material ASAR MP4 in self-cure (SC) and light-cure (LC) mode. ASAR MP4 was processed in capsules. Three direct resin composites (CeramX mono+, DentsplySirona; Heliomolar, IvoclarVivadent; Filtek Supreme XTE, 3M) and two glass-ionomer-cement (GIC) based materials (Equia Forte, GC; Fuji II LC, GC) were selected for comparison with ASAR MP4. FS specimens (n = 15) were tested in a 4-point bending configuration according to ISO 4049 and 9917. FFS specimens (n = 25) were additionally stressed for 104 loading cycles using the staircase approach. The single-edge-notch beam (SENB) configuration was selected for determining KIc according to ISO 13586. All specimens were stored for 14 days at 37°C. Data were analyzed using Weibull statistics (FS), ANOVA (FS, KIc), and the non-parametric Mann-Whitney U-test (FFS).
RESULTS: The FS, FFS and KIc data of the ASAR MP4 material reveal a mechanical performance in the range of the successful permanent direct resin composites CeramX mono+ and Heliomolar. The results for ASAR MP4 in SC mode were superior to the LC mode. A fine-grained and pore-free microstructure was observed.
CONCLUSION: Within the limitations of this study we conclude that the novel self-adhesive restorative material ASAR MP4 exhibits mechanical performance close to that of the resin composites Heliomolar and CeramX mono+, both indicated for permanent use in the load-bearing posterior region. Processing the material in either self-cure or light-cure mode led to superior performance over glass-ionomer cements.

Entities:  

Keywords:  cyclic fatigue; fracture toughness; glass-ionomer cement; resin composite; self-adhesion; flexural strength

Mesh:

Substances:

Year:  2020        PMID: 32030375     DOI: 10.3290/j.jad.a43997

Source DB:  PubMed          Journal:  J Adhes Dent        ISSN: 1461-5185            Impact factor:   2.359


  3 in total

1.  Evaluation of the Behavior of Two CAD/CAM Fiber-Reinforced Composite Dental Materials by Immersion Tests.

Authors:  Farah Bechir; Simona Maria Bataga; Adrian Tohati; Elena Ungureanu; Cosmin Mihai Cotrut; Edwin Sever Bechir; Mircea Suciu; Diana Maria Vranceanu
Journal:  Materials (Basel)       Date:  2021-11-25       Impact factor: 3.623

2.  Methacrylate peak determination and selection recommendations using ATR-FTIR to investigate polymerisation of dental methacrylate mixtures.

Authors:  António H S Delgado; Anne M Young
Journal:  PLoS One       Date:  2021-06-09       Impact factor: 3.240

3.  One-year clinical results of restorations using a novel self-adhesive resin-based bulk-fill restorative.

Authors:  Andreas Rathke; Frank Pfefferkorn; Michael K McGuire; Rick H Heard; Rainer Seemann
Journal:  Sci Rep       Date:  2022-03-10       Impact factor: 4.379

  3 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.