| Literature DB >> 31138808 |
Xiuquan Jia1, Jiping Ma2, Fei Xia1,3, Mingxia Gao1,3, Jin Gao1, Jie Xu4.
Abstract
The design of metal oxide catalysts predominantly focuses on the composition or geometry engineering to enable optimized reactivity on the surface. Despite the numerous reports investigating the surface chemisorption of organic molecules onEntities:
Year: 2019 PMID: 31138808 PMCID: PMC6538668 DOI: 10.1038/s41467-019-10315-9
Source DB: PubMed Journal: Nat Commun ISSN: 2041-1723 Impact factor: 14.919
The catalytic performance of manganese oxide catalysts in the benzylamine aerobic oxidation reaction
|
| |||||
|---|---|---|---|---|---|
| Entry | Cat. | Mass-specific activity (mmol gcat−1 h−1) | Conv. (%) | Yield (%) | |
| 2a | 3a | ||||
| 1 | α-MnO2 | 45.4 ± 2.1 | 94.5 ± 0.4 | 47.9 ± 2.4 | 44.6 ± 3.1 |
| 2 | γ-MnO2 | 61.8 ± 4.0 | 97.4 ± 0.2 | 58.6 ± 4.4 | 32.5 ± 3.7 |
| 3 | δ-MnO2 | 15.7 ± 0.7 | 94.9 ± 0.1 | 61.9 ± 3.0 | 24.6 ± 5.0 |
| 4 | OMS-2 | 63.4 ± 5.2 | 93.1 ± 0.2 | 24.1 ± 2.6 | 58.9 ± 2.0 |
| 5 | MnOx | 129.2 ± 4.2 | >99 | 0 | 86.5 ± 0.3 |
| 6a | MnOx | — | >99 | 7.0 ± 1.2 | 80.1 ± 1.0 |
| 7a, b | MnOx | — | 93.0 ± 0.2 | 46.7 ± 0.2 | 41.2 ± 2.5 |
| 8 | acac-MnOx | 14.7 ± 1.9 | 94.1 ± 0.3 | 90.6 ± 4.1 | 3.4 ± 0.2 |
Reaction conditions: 1 mmol Benzylamine, 0.1 mmol catalyst, acac/MnOx = 20 mol% for acac-MnOx, 5 mL CH3CN, 0.3 MPa O2, 90 °C, 14 h.
a0.05 mmol MnOx
b60 °C
Fig. 1Performance of MnOx with different modifiers in the aerobic oxidation of benzylamine. Reaction conditions: 1 mmol benzylamine, 0.1 mmol MnOx, additive/MnOx = 20 mol%, 5 mL CH3CN, 0.3 MPa O2, 90 °C, 14 h. a20 h. bAdditive/MnOx = 200 mol%
Fig. 2Catalyst characterization. a FT-IR spectra of acac and acac-MnOx after evacuation at 150 °C for 0.5 h. b FT-IR spectra of pyridine adsorption to MnOx and acac-MnOx
Fig. 3Reactivity of N-benzylidenebenzylamine (2a) over unmodified and acac-modified MnOx. a Mass-specific activities (mmol gcat−1 h−1) of MnOx and acac-MnOx in aerobic oxidation/ammoxidation of N-benzylidenebenzylamine (2a) under 0.3 MPa O2 at 90 °C. The mass-specific activity was measured at the reaction time of 1 h when the conversion is below 30%. b Selectivity-conversion correlation of N-benzylidenebenzylamine (2a) in aerobic oxidation of benzylamine under 0.3 MPa O2 at 90 °C. c Proposed mechanism. d Recyclability test results for selective synthesis of N-benzylidenebenzylamine (2a) by oxidation of benzylamine over acac modified MnOx. Reaction conditions: 1 mmol benzylamine, 0.1 mmol MnOx, acac/MnOx = 20 mol%, 5 mL CH3CN, 0.3 MPa O2, 90 °C, 14 h
Fig. 4Synthesis of nitriles and imines using benzylamine derivatives over unmodified and acac-modified MnOx. Reaction conditions: 1 mmol benzylamine, 0.1 mmol MnOx, acac/MnOx = 20 mol% for acac-MnOx, 5 mL CH3CN, 0.3 MPa O2, 90 °C, 14 h