Literature DB >> 30293020

Influential parameters on natural weathering under harsh climatic conditions of mechanically recycled plastic film specimens.

S M Al-Salem1.   

Abstract

In this work, real life reclaimed plastic solid waste (PSW) secured from the municipal sector was mechanically recycled and compounded with virgin linear low density polyethylene (LLDPE). The compounding of the plastic film samples utilised the means of extrusion and blown filming to produce various formulations of the blends containing up to 100% (by weight) of the PSW in the examined specimens. The film samples were compared to market products used in the State of Kuwait where PSW accumulation presents a major obstacle. Natural weathering under arid and harsh climatic conditions was also performed to determine the degradation extent of the film samples. Haze (%), light transmission (%) and the total change in colour (ΔE) were measured as indicators to the degradation profile of the polymeric materials, in addition to tensile pull mechanical properties. Properties were noted to deteriorate as a function of weathering time and waste content. Statistical analysis was also performed on the properties measured and climatic conditions including airborne pollutants levels. The abundance of the secondary airborne pollutant (ozone) was determined to be a significant variable on the studied properties. This can be attributed to induced photo-oxidation the polymeric matrix is subjected to under such climatic conditions which increases oxygen diffusion throughout the polymeric matrix. Future development of the recycled blends studied in this work can be a route for the decrease of associated environmental stressors with virgin plastic resin conversion.
Copyright © 2018 Elsevier Ltd. All rights reserved.

Entities:  

Keywords:  ANOVA; Plastic waste; Recycling; Waste management; Weathering

Mesh:

Substances:

Year:  2018        PMID: 30293020     DOI: 10.1016/j.jenvman.2018.09.044

Source DB:  PubMed          Journal:  J Environ Manage        ISSN: 0301-4797            Impact factor:   6.789


  3 in total

1.  On the Kinetics of Degradation Reaction Determined Post Accelerated Weathering of Polyolefin Plastic Waste Blends.

Authors:  S M Al-Salem; M H Behbehani; H J Karam; S F Al-Rowaih; F M Asiri
Journal:  Int J Environ Res Public Health       Date:  2019-01-30       Impact factor: 3.390

2.  Thermal and Rheological Characterization of Recycled PET/Virgin HDPE Blend Compatibilized with PE-g-MA and an Epoxy Chain Extender.

Authors:  Raquel M Santos; Anna R M Costa; Yêda M B Almeida; Laura H Carvalho; João M P Q Delgado; Elisiane S Lima; Hortência L F Magalhães; Ricardo S Gomez; Boniek E Leite; Fagno D Rolim; Maria J Figueiredo; Antonio G B Lima
Journal:  Polymers (Basel)       Date:  2022-03-12       Impact factor: 4.329

3.  Separation of virgin plastic polymers and post-consumer mixed plastic waste by sinking-flotation technique.

Authors:  Washington Orlando Meneses Quelal; Borja Velázquez-Martí; Andrés Ferrer Gisbert
Journal:  Environ Sci Pollut Res Int       Date:  2021-08-05       Impact factor: 4.223