Effects of silver diammine fluoride on bond strength of adhesives to sound dentin.

Paul Lutgen1, Daniel Chan2, Alireza Sadr2,3.   

Abstract

This study evaluated bonding of adhesives to dentin treated with silver diammine fluoride (SDF). Micro-shear bond strength (MSBS) to sound human dentin was investigated for 3 adhesive systems: Clearfil SE bond 2 (CSE), and Scotchbond Universal in self-etching (SBU) and phosphoric acid-etching (SBT) modes, following 4 different SDF application protocols (n=10); Control: treated with deionized water. P1: SDF applied for 10-s, no rinse. P2: SDF applied for 10-s, rinsed off after 1-min. P3: superficial dentin polished off after 24-h following P1. MSBS data were obtained after 24-h water storage at 37°C. SDF significantly affected MSBS to dentin depending on the SDF protocol and adhesive system. Rinsing SDF off improved bond strength but superficial refreshing of SDFtreated dentin prior to bonding showed the highest bond strength. The two-step self-etch adhesive (CSE) and the universal adhesive in acid-etching mode (SBT) showed better performance than universal adhesive (SBU) alone on SDF treated dentin.

Entities:  

Keywords:  Dentin bond strength; Self-etching; Silver diammine fluoride; Total-etching; Universal adhesive

Mesh:

Substances:

Year:  2018        PMID: 30224603     DOI: 10.4012/dmj.2017-401

Source DB:  PubMed          Journal:  Dent Mater J        ISSN: 0287-4547            Impact factor:   2.102


  4 in total

1.  Remineralization of caries-affected dentin and color stability of teeth restored after treatment with silver diamine fluoride and bioactive glass-ceramic.

Authors:  Adriana Cavalcanti Ferreira; Rebeca Franco de Lima Oliveira; Ayodele Alves Amorim; Rocio Geng-Vivanco; Fernanda de Carvalho Panzeri Pires-de-Souza
Journal:  Clin Oral Investig       Date:  2022-03-17       Impact factor: 3.606

2.  Effect of silver diamine fluoride solution application on the bond strength of dentine to adhesives and to glass ionomer cements: a systematic review.

Authors:  Meng Jiang; May Lei Mei; May Chun Mei Wong; Chun Hung Chu; Edward Chin Man Lo
Journal:  BMC Oral Health       Date:  2020-02-05       Impact factor: 2.757

3.  Investigation of the effect of simultaneous use of silver diamine fluoride and potassium iodide on the shear bond strength of total etch and universal adhesive systems to dentin.

Authors:  Farnaz Farahat; Abdolrahim Davari; Haleh Karami
Journal:  Dent Res J (Isfahan)       Date:  2022-01-28

4.  Evaluation of the Effect of the Loading Time on the Microtensile Bond Strength of Various Restorative Materials Bonded to Silver Diamine Fluoride-Treated Demineralized Dentin.

Authors:  Mohammed M Aldosari; Fares S Al-Sehaibany
Journal:  Materials (Basel)       Date:  2022-06-23       Impact factor: 3.748

  4 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.